使用三维测量技术评估光固化和自凝重衬材料的贴合精度

Evaluation of Fitting Accuracy of Light- and Auto-Polymerizing Reline Materials Using Three-Dimensional Measurement Techniques.

作者信息

Utsumi Miona, Murakami Natsuko, Yamazaki Toshiki, Hirata Asuka, Komine Kohei, Li Bin, Takakusaki Kensuke, Wada Junichiro, Wakabayashi Noriyuki

机构信息

Department of Advanced Prosthodontics, Institute of Science Tokyo, Tokyo 113-8510, Japan.

出版信息

Polymers (Basel). 2025 Jan 15;17(2):201. doi: 10.3390/polym17020201.

Abstract

Light-polymerizing reline materials offer improved chairside workability compared to conventional auto-polymerizing reline materials, addressing the partial denture (RPD) incompatibility caused by residual ridge resorption owing to long-term use. This study evaluates the fitting accuracy of relined materials by combining conventional fitting tests with three-dimensional (3D) measurements for detailed analysis. Light-polymerizing reline material (HikariLiner, Tokuyama, Tokyo, Japan, LP) and auto-polymerizing material (Rebase III, Tokuyama, AP) were used. The gaps formed between the relined denture base and the simplified edentulous model were evaluated. The displacement and deviation of the experimentally relined RPDs on the partially edentulous models were analyzed using 3D data superimposition. In the edentulous model, the gaps at all measurement points were significantly smaller for the AP than in the LP. Moreover, the alveolar ridge crest gap was significantly larger than that at other sites. In the partial denture model, the RMS values at the residual ridge crest were significantly lower for the AP. The evaluation method using 3D scanning and comparison was suitable for a detailed fit analysis. Further improvements in the scanning accuracy may enhance future assessments. Therefore, the evaluation method using 3D scanning and comparison was suitable for effectively analyzing the fit of relines, necessitating further accuracy improvements.

摘要

与传统的自凝重衬材料相比,光固化重衬材料具有更好的椅旁操作性,可解决长期使用导致的残余牙槽嵴吸收引起的局部义齿(RPD)不匹配问题。本研究通过将传统的贴合测试与三维(3D)测量相结合进行详细分析,评估重衬材料的贴合精度。使用了光固化重衬材料(HikariLiner,日本东京德山公司,LP)和自凝材料(Rebase III,德山公司,AP)。评估了重衬义齿基托与简化无牙颌模型之间形成的间隙。使用3D数据叠加分析了实验性重衬RPD在部分无牙颌模型上的位移和偏差。在无牙颌模型中,AP在所有测量点的间隙均明显小于LP。此外,牙槽嵴顶间隙明显大于其他部位。在局部义齿模型中,AP在残余牙槽嵴顶的RMS值明显更低。使用3D扫描和比较的评估方法适用于详细的贴合分析。扫描精度的进一步提高可能会增强未来的评估。因此,使用3D扫描和比较的评估方法适用于有效分析重衬的贴合情况,需要进一步提高精度。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/1567/11769256/19e85deac4d8/polymers-17-00201-g001.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验