Suppr超能文献

[不同含水量水凝胶角膜假体的动物实验经验]

[Experiences in animal experiments with hydrogel keratoprosthesis of different water content].

作者信息

Mester U

出版信息

Ophthalmologica. 1979;179(1):62-9. doi: 10.1159/000308865.

Abstract

Satisfactory results could be obtained in former animal experiments with keratoprostheses made by 38% hydrated hydrogel plastics (PHEMA). There still existed some doubts concerning alterations by aging of this material, possibly resulting in setting free toxic or allergenic substances as well as raising the risk of infection. Therefore, keratoprostheses containing 38 or 20% water were implanted in rabbit eyes. The follow-up period of 44 animals was 6 months. No essential differences in the postoperative course of both types of keratoprostheses could be observed. With the only exception of a growth of tissue over the optical cylinder in 1 case no serious complications, e.g., extrusion of the implant, occurred. Regarding the greater resistibility of the less hydrated hydrogel, this more durable plastic seems to be the more adapted material for keratoprotheses.

摘要

在之前用38%水合水凝胶塑料(聚甲基丙烯酸羟乙酯)制成的人工角膜进行的动物实验中可获得满意结果。对于这种材料因老化而发生的变化仍存在一些疑问,这可能会导致释放有毒或致敏物质以及增加感染风险。因此,将含水量为38%或20%的人工角膜植入兔眼。44只动物的随访期为6个月。两种类型的人工角膜术后过程未观察到本质差异。除1例在光学柱体上有组织生长外,未发生严重并发症,如植入物挤出。鉴于含水量较低的水凝胶具有更大的抵抗力,这种更耐用的塑料似乎是更适合用于人工角膜的材料。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验