温度和相对湿度对牙本质早期粘结强度的影响。

Influence of temperature and relative humidity on early bond strengths to dentine.

作者信息

Burrow M F, Taniguchi Y, Nikaido T, Satoh M, Inai N, Tagami J, Takatsu T

机构信息

Tokyo Medical and Dental University, Department of Operative Dentistry, Japan.

出版信息

J Dent. 1995 Feb;23(1):41-5. doi: 10.1016/0300-5712(95)90659-6.

Abstract

The effect of temperature and relative humidity (RH) on the early tensile bond strengths to bovine dentine of two bonding systems (Liner Bond System, and Scotchbond Multi-purpose), and an experimental system (KB-110) were tested. Two environmental conditions, room temperature (23 degrees C/50% RH) and oral temperature (30 degrees C/80% RH), were used in a controlled temperature and humidity chamber. Bond strengths were recorded immediately after, 10 min and 24 h following light curing. The tensile bond strengths did not vary between the two test conditions, but the mode of fracture was observed to change. The 30 degrees C/80% RH condition exhibited a slightly greater degree of adhesive type failures compared with the 23 degrees C/50% RH group. This was particularly so for the experimental system, indicating that different bonding systems may be more or less sensitive to changes in RH and temperature. Failures occurred partially or totally within the resin composite at the early test times, and it was concluded that the bond strengths of the systems tested tended to exceed the early cohesive strengths of the resin composite.

摘要

测试了温度和相对湿度(RH)对两种粘结系统(线性粘结系统和多功能思高粘结剂)以及一种实验系统(KB - 110)与牛牙本质早期拉伸粘结强度的影响。在可控温湿度试验箱中采用两种环境条件,即室温(23℃/50%RH)和口腔温度(30℃/80%RH)。在光固化后即刻、10分钟和24小时记录粘结强度。两种测试条件下的拉伸粘结强度没有差异,但观察到断裂模式发生了变化。与23℃/50%RH组相比,30℃/80%RH条件下表现出稍高程度的粘结剂型失败。实验系统尤其如此,表明不同的粘结系统对RH和温度变化的敏感程度可能或多或少有所不同。在早期测试时间,失败部分或全部发生在树脂复合材料内部,并且得出结论,所测试系统的粘结强度往往超过树脂复合材料的早期内聚强度。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验