Kissmeyer-Nielsen P, Christensen H, Laurberg S
Department of Surgery L, University Hospital of Aarhus, Denmark.
Int J Colorectal Dis. 1993 Sep;8(3):120-4. doi: 10.1007/BF00341182.
The effects of a diverting colostomy on weight, collagen content, and biomechanical strength of the left colon was investigated in rats. Female rats received either a diverting colostomy or a sham-operation and were killed randomly 1, 2, 4, or 12 weeks after surgery. The dry weight and hydroxyproline content of excluded colon decreased by 37% (P < 0.001, confidence limits (CL) = 21-53%) and 25% (P < 0.001, CL = 18-31%), respectively, after 4 weeks, and by 52% (P < 0.001, CL = 38-66%) and 40% (P < 0.001, CL = 27-53%), respectively, after 12 weeks compared to sham-operated rats. The breaking strength of the defunctioned colon decreased by 21% (P < 0.05, CL = 2-40%) after 4 weeks and by 25% after 12 weeks (P < 0.05, CL = 4-46%). The tensile strength of defunctioned colon (load per unit collagen) was reduced by 19% after 4 weeks (P < 0.05, CL = 6-32%). Proximal to the colostomy site we found no differences in the hydroxyproline content or biomechanical strength. In conclusion, defunctioning of the left colon in rats leads to deterioration in the biomechanical properties caused by a lesser content and a decreased quality in the collagen of the left colon.
在大鼠中研究了转流性结肠造口术对左半结肠重量、胶原蛋白含量和生物力学强度的影响。雌性大鼠接受转流性结肠造口术或假手术,并在术后1、2、4或12周随机处死。与假手术大鼠相比,4周后,旷置结肠的干重和羟脯氨酸含量分别下降了37%(P<0.001,置信区间(CL)=21%-53%)和25%(P<0.001,CL=18%-31%),12周后分别下降了52%(P<0.001,CL=38%-66%)和40%(P<0.001,CL=27%-53%)。失功能结肠的断裂强度在4周后下降了21%(P<0.05,CL=2%-40%),12周后下降了25%(P<0.05,CL=4%-46%)。失功能结肠的拉伸强度(单位胶原蛋白的负荷)在4周后降低了19%(P<0.05,CL=6%-32%)。在结肠造口部位近端,我们发现羟脯氨酸含量或生物力学强度没有差异。总之,大鼠左半结肠失功能会导致生物力学性能恶化,这是由左半结肠胶原蛋白含量减少和质量下降引起的。