用作根尖倒充填材料的各种银汞合金产品的封闭性评估。

Evaluation of the seal of various amalgam products used as root-end fillings.

作者信息

Johnson J R, Anderson R W, Pashley D H

机构信息

Department of Endodontics, School of Dentistry, Meical College of Georgia, Augusta, GA 30912, USA.

出版信息

J Endod. 1995 Oct;21(10):505-8. doi: 10.1016/s0099-2399(06)80522-4.

Abstract

Different formulations of amalgam have physical properties that may make them behave differently in the often-contaminated root end environment. Five different brands of amalgam were evaluated for microleakage of root-end fillings placed in extracted human teeth. These included a zinc-free spherical amalgam, a zinc-free admixture amalgam, two zinc-containing admixture amalgams, and a zinc-containing lathe-cut amalgam. The amalgams were placed either into dry root-end preparations or into preparations contaminated with human blood. The fluid filtration method was used to measure microleakage at 1, 2, 4, 8, 12, and 24 wk after placement. Analysis of variance revealed significant differences in the rates of microleakage at every measurement period. Scheffé's test showed that the zinc-free spherical amalgam had significantly greater leakage than all the other products evaluated. There were no significant differences between any of the other products. Blood contamination did not adversely affect the seal of any amalgam.

摘要

不同配方的汞合金具有一些物理特性,这些特性可能使它们在常常受到污染的根尖环境中的表现有所不同。对五种不同品牌的汞合金进行了评估,以检测置于拔除的人牙中的根尖充填物的微渗漏情况。这些汞合金包括一种无锌球形汞合金、一种无锌混合型汞合金、两种含锌混合型汞合金和一种含锌车削型汞合金。将这些汞合金分别置于干燥的根尖预备洞中或被人血污染的预备洞中。采用液体过滤法在充填后1周、2周、4周、8周、12周和24周测量微渗漏情况。方差分析显示在每个测量时间段微渗漏率存在显著差异。谢费检验表明,无锌球形汞合金的渗漏明显大于所评估的所有其他产品。其他任何产品之间均无显著差异。血液污染并未对任何汞合金的封闭性产生不利影响。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验