Suppr超能文献

Clearfil Liner Bond 2的粘结强度及扫描电子显微镜评估

Bond strengths and SEM evaluation of Clearfil Liner Bond 2.

作者信息

Barkmeier W W, Los S A, Triolo P T

机构信息

Creighton University School of Dentistry, Omaha, NE 68178, USA.

出版信息

Am J Dent. 1995 Dec;8(6):289-93.

PMID:8695004
Abstract

PURPOSE

To evaluate a dental adhesive system that uses a single conditioning/primer agent.

MATERIALS AND METHODS

Twenty-five flat enamel and dentin bonding sites were prepared to 600 grit on human molar teeth. The Clearfil Liner Bond 2 adhesive system was used to bond Clearfil AP-X composite to both enamel and dentin. After 24 hours of water storage, shear bond strengths were determined using an Instron testing machine. Fifty V-shaped cavity preparations were prepared in human molar teeth with an enamel and cementum margin. Composite restorations were placed using the new adhesive system. The teeth were stored for 24 hours, thermocycled, stained with AgNO3 , sectioned and examined for microleakage. SEM examinations were also completed to evaluate the effects of the treatment steps on enamel and dentin surfaces.

RESULTS

Mean shear bond strengths for the experimental adhesive to enamel and dentin were 28.2 +/- 4.9 and 19.4 +/- 3.1 MPa. A t-test revealed that the enamel bond strength was significantly greater (P<0.05) than the dentin strength. No marginal leakage was observed from the enamel margins of the restorations. Three restorations showed minimal leakage from the cementum margins. SEM examinations showed resin penetration into both the conditioned enamel and dentin surfaces. The adhesive system produced high bond strengths to both enamel and dentin, exhibited very minimal microleakage and was easy to use.

摘要

目的

评估一种使用单一调理/底漆剂的牙科粘结系统。

材料与方法

在人类磨牙上制备25个平面釉质和牙本质粘结部位,打磨至600目。使用Clearfil Liner Bond 2粘结系统将Clearfil AP-X复合材料粘结到釉质和牙本质上。储水24小时后,使用Instron试验机测定剪切粘结强度。在人类磨牙上制备50个具有釉质和牙骨质边缘的V形洞型。使用新的粘结系统进行复合树脂修复。牙齿储存24小时,进行热循环处理,用硝酸银染色,切片并检查微渗漏情况。还完成了扫描电子显微镜检查,以评估处理步骤对釉质和牙本质表面的影响。

结果

实验粘结剂对釉质和牙本质的平均剪切粘结强度分别为28.2±4.9和19.4±3.1MPa。t检验显示,釉质粘结强度显著高于牙本质强度(P<0.05)。修复体的釉质边缘未观察到边缘渗漏。三个修复体的牙骨质边缘显示出最小程度的渗漏。扫描电子显微镜检查显示树脂渗入了经处理的釉质和牙本质表面。该粘结系统对釉质和牙本质均产生了高粘结强度,微渗漏极少,且易于使用。