Improved techniques in preparing and sizing dental alloy powders containing Ag, Sn, and Cu have led to amalgams with higher strengths and less spread in dimensional change but very poor shelf life. Since maximum strengths occurred for amalgams containing about 15% more Sn than previously reported, and consequently presumably more of the weak gamma2 phase, the higher strengths are difficult to understand. The poor shelf life may be explained by oxidation of the highly reactive splat-cooled alloy or possibly by the existence of highly reactive metastable phases which transform fairly rapidly to the less reactive equilibrium ones.

摘要

在制备和筛选含银、锡和铜的牙科合金粉末方面的改进技术,已产生了强度更高、尺寸变化扩散更小但保质期极短的汞齐合金。由于含锡量比先前报道的大约多15%的汞齐合金出现了最大强度,因此推测可能存在更多的弱γ2相,所以较高的强度难以理解。保质期短可能是由于快速凝固冷却合金的氧化,或者可能是由于存在高活性亚稳相,这些亚稳相相当迅速地转变成活性较低的平衡相。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验