Berry E A, Powers J M
University of Texas-Houston Health Science Center, Department of Basic Sciences/Oral Biomaterials 77225, USA.
Oper Dent. 1994 Jul-Aug;19(4):122-6.
A study was conducted to compare the shear bond strength of a glass-ionomer cement and glass-ionomer base to coronal and radicular dentin. Two different glass ionomers were bonded to paired coronal and radicular human dentin surfaces that had received no surface treatment or had been treated passively for 20 seconds with either 40% or 25% polyacrylic acid. When only the effect of the type of dentin surface was considered, glass-ionomer bonds were greater to radicular dentin than to coronal dentin. With one exception, bond strengths to both dentin surfaces were greater with the base ionomer (Ketac-Bond) than with the luting cement (Ketac-Cem). Bond strengths of both glass ionomers were greater after dentin surface treatment with either 25% or 40% polyacrylic acid than with no treatment.
开展了一项研究,以比较玻璃离子水门汀和玻璃离子基底与冠部和根部牙本质之间的剪切粘结强度。将两种不同的玻璃离子粘结到成对的未进行表面处理或用40%或25%聚丙烯酸被动处理20秒的人类冠部和根部牙本质表面。仅考虑牙本质表面类型的影响时,玻璃离子与根部牙本质的粘结力大于与冠部牙本质的粘结力。除了一个例外,基底离子水门汀(Ketac-Bond)与两种牙本质表面的粘结强度均高于粘结水门汀(Ketac-Cem)。用25%或40%聚丙烯酸对牙本质表面进行处理后,两种玻璃离子的粘结强度均高于未处理时。