Theodoridou-Pahini S, Tolidis K, Papadogiannis Y
Department of Operative Dentistry, Aristotle University of Thessaloniki, Greece.
Int J Paediatr Dent. 1996 Sep;6(3):173-6. doi: 10.1111/j.1365-263x.1996.tb00237.x.
The purpose of this study was to evaluate and compare the degree of microleakage exhibited by five resin sealants (Concise, Helioseal, Durafil. Fissurit, Sci-Pharm) and a glass-ionomer sealant (Fuji Glass lonomer Type III). The fissure systems of the occlusal surfaces of freshly extracted teeth were opened using a pear-shaped bur; the preparations were confined to enamel. For each material, 14 teeth were prepared. From each group, seven teeth were thermocycled through 5 degrees, 37 degrees, 60 degrees and 37 degrees for 2000 cycles, and the other seven teeth were not thermocycled. All teeth were immersed in 0.5% solution of basic fuchsin dye for 48 hours. Each tooth was sectioned longitudinally in the buccolingual direction and three 1 mm-thick sections (distal, central and proximal) were obtained from each tooth. Each section was cleaned, examined, and photographed in a stereomicroscope. All the materials presented microleakage in both the thermocycled and non-thermocycled specimens; the degree of microleakage was greater in the thermocycled specimens. The results support the practice of opening up questionably carious fissures and removing caries (if present) before sealing.
本研究的目的是评估和比较五种树脂封闭剂(Concise、Helioseal、Durafil、Fissurit、Sci-Pharm)和一种玻璃离子封闭剂(富士III型玻璃离子)的微渗漏程度。使用梨形车针打开新鲜拔除牙齿咬合面的裂隙系统;制备仅限于牙釉质。每种材料制备14颗牙齿。每组中,7颗牙齿在5℃、37℃、60℃和37℃之间进行2000次热循环,另外7颗牙齿不进行热循环。所有牙齿浸泡在0.5%碱性品红染料溶液中48小时。每颗牙齿沿颊舌方向纵向切开,从每颗牙齿获取三个1毫米厚的切片(远中、中央和近中)。每个切片进行清洁、检查,并在体视显微镜下拍照。所有材料在热循环和未热循环的标本中均出现微渗漏;热循环标本中的微渗漏程度更大。结果支持在封闭前打开可疑龋裂并去除龋坏(如有)的做法。