Fellner C, Behr M, Fellner F, Held P, Handel G, Feuerbach S
Institut für Röntgendiagnostik, Klinikum der Universität Regensburg.
Rofo. 1997 May;166(5):421-8. doi: 10.1055/s-2007-1015452.
The influence of dental alloys on MRI of the temporomandibular joint was studied using a phantom model for this joint.
At 1,5 T, 15 dental alloys and 14 of their most important components were investigated acquiring sagittal (FOV: 150 mm) and transverse (FOV: 250 mm) T1-weighted SE images. In 11 cases, T1- and T2*-weighted FLASH images were measured additionally. The artifacts were assessed qualitatively as well as quantitatively, and the samples were subdivided into four artifact categories.
Ag, Cu, Ga, In, Tl, Sn, Zn, amalgam, the precious alloys, the Au-Pd and Ag-Pd alloys showed no artifacts (category I). Minimal artifacts below 10 mm on transverse images (category II) were found for Cr, Pd, Pt and for the Ni-Cr alloy. Mn and the remaining non-precious alloys induced artifacts up to 30 mm (category III). Significant artifacts-more than 30 mm-(category IV) were caused by Ni-Cr and 18/8 wires and by Co, Fe, and Ni. T2*-weighted FLASH proved to be more susceptible for artifacts than T1-weighted SE and FLASH techniques.
In contrast to dental alloys for fixed prosthodontics, Ni-Cr- or 18/8 wires used for orthodontic bands can influence not only the image quality, but also the diagnostic reliability of MRI of the temporomandibular joint.
使用颞下颌关节模型研究牙科合金对颞下颌关节磁共振成像(MRI)的影响。
在1.5T磁场下,对15种牙科合金及其14种最重要的成分进行研究,采集矢状位(视野:150mm)和横断位(视野:250mm)T1加权自旋回波(SE)图像。在11例中,还测量了T1加权和T2*加权快速低角度激发(FLASH)图像。对伪影进行定性和定量评估,并将样本分为四类伪影。
银、铜、镓、铟、铊、锡、锌、汞合金、贵金属合金、金钯合金和银钯合金未显示伪影(I类)。在横断位图像上发现铬、钯、铂和镍铬合金有小于10mm的轻微伪影(II类)。锰和其余非贵金属合金产生的伪影长达30mm(III类)。镍铬合金、18/8钢丝、钴、铁和镍导致显著伪影(超过30mm)(IV类)。T2*加权FLASH序列比T1加权SE和FLASH序列对伪影更敏感。
与固定修复用牙科合金不同,正畸带环使用的镍铬合金或18/8钢丝不仅会影响图像质量,还会影响颞下颌关节MRI的诊断可靠性。