Sepet E, Aytepe Z, Oray H
Department of Pedodontics, Faculty of Dentistry, University of Istanbul, Turkey.
J Clin Pediatr Dent. 1997 Spring;21(3):231-5.
The aim of this study was to investigate the surface texture and enamel-restoration interface of Class II glass ionomer restorations in primary molars. A traditional (Chemfil II), a cermet (Chelon-Silver) cement and two light cured glass ionomer cements (Vitremer and Dyract) were used to restore the Class II cavities of 20 primary molars. The surface changes and enamel-restoration interface of restorative materials were evaluated by SEM, after a 12 month period. Microcracks and pores in surface were observed in all of the four different glass ionomer materials. Although, there was no marginal gap formation for Chemfil II, Chelon-Silver and Dyract samples, in 2 samples of Vitremer group gap formation was found with an ion-exchange layer. Also, in Dyract samples wear of restorations was considerable.
本研究的目的是调查乳牙Ⅱ类玻璃离子修复体的表面纹理及牙釉质-修复体界面。使用一种传统材料(Chemfil II)、一种金属陶瓷材料(Chelon-Silver)黏固粉以及两种光固化玻璃离子黏固粉(Vitremer和Dyract)对20颗乳牙的Ⅱ类洞进行修复。12个月后,通过扫描电子显微镜(SEM)评估修复材料的表面变化及牙釉质-修复体界面。在所有四种不同的玻璃离子材料中均观察到表面存在微裂纹和孔隙。尽管Chemfil II、Chelon-Silver和Dyract样本未形成边缘间隙,但在Vitremer组的2个样本中发现有离子交换层形成间隙。此外,Dyract样本的修复体磨损相当严重。