Dean J A, Minutillo A L, Moore B K
Department of Oral Facial Development, Indiana University School of Dentistry, USA.
Pediatr Dent. 1998 Jan-Feb;20(1):49-52.
The purpose of this study was to compare the dislodgement strengths and fracture types for reattached tooth fragments using a light-cured composite resin material, a hybrid light-cured glass ionomer base, and a hybrid light-cured glass ionomer liner.
Seventy-five bovine incisor teeth were fractured, randomly divided into three groups of equal number, and then luted back together with three different materials (Universal Bonding Agent/TPH Composite Resin; VariGlass VLC Base; and VariGlass VLC Liner: LD Caulk Div Dentsply Int Inc, Milford, DE). The reattached fragments were subjected to thermocycling with a 40 degrees C differential and then were loaded until the force required to dislodge the fragment was reached.
The mean dislodgement strengths were 36.8 (+/- 25.6) kg for the composite resin, 36.4 (+/- 26.7) kg for the glass ionomer base, and 31.4 (+/- 29.5) kg for the glass ionomer liner. Cohesive fractures occurred in 73% of the dislodgements.
There was no statistically significant difference demonstrated (P < 0.05) between the three groups in terms of both dislodgement strength and fracture type.
本研究旨在比较使用光固化复合树脂材料、混合型光固化玻璃离子垫底材料和混合型光固化玻璃离子衬层材料重新附着牙碎片的脱位强度和骨折类型。
将75颗牛切牙折断,随机分为三组,每组数量相等,然后用三种不同材料(通用粘结剂/TPH复合树脂;VariGlass VLC垫底材料;VariGlass VLC衬层材料:LD Caulk Div Dentsply Int Inc,米尔福德,特拉华州)重新粘结在一起。对重新附着的碎片进行40℃温差的热循环处理,然后加载直至达到使碎片脱位所需的力。
复合树脂的平均脱位强度为36.8(±25.6)kg,玻璃离子垫底材料为36.4(±26.7)kg,玻璃离子衬层材料为31.4(±29.5)kg。73%的脱位发生粘结性骨折。
三组在脱位强度和骨折类型方面均未显示出统计学上的显著差异(P < 0.05)。