Evaluation of coronal microleakage of four different glass-ionomer cements in endodontically treated teeth.

作者信息

Görgül G, Dolar K, Uçtaşli M, Tinaz C, Cankaya F, Kinoğlu T

机构信息

Department of Endodontics and Operative Dentistry, Gazi University, Faculty of Dentistry, Ankara, Türkiye.

出版信息

J Marmara Univ Dent Fac. 1996 Sep;2(2-3):546-50.

PMID:9569814
Abstract

Four different glass-ionomer materials were evaluated for coronal microleakage in permanent lingual access restorations of endodontically treated anterior teeth. Forty extracted human anterior teeth were randomly divided into four groups following chemomechanical preparations and obturations with gutta-percha and sealer. Logobond, Aqua Ionobond, Ionoseal and Ketac-Cem were placed in 2 mm thickness over the gutta-percha obturation from cemento-enamel junction. Eight teeth were used as negative and positive controls. The teeth were thermocycled, coated with nail varnish and paraffin except around the access preparation. Next they were placed in dye and cleared to allow visualization of dye penetration. There was a tendency for the Ketac-Cem group to lack least but there were no statistically differences among the groups.

摘要

对四种不同的玻璃离子材料进行了评估,以研究其在牙髓治疗的前牙永久性舌侧通路修复体中的冠部微渗漏情况。40颗拔除的人前牙在进行化学机械预备并用牙胶和封闭剂充填后,随机分为四组。将乐固邦、水离子粘结剂、离子封闭剂和凯塔胶结剂在距牙骨质-釉质界处的牙胶充填物上方以2毫米的厚度放置。8颗牙齿用作阴性和阳性对照。牙齿经过热循环处理,除通路预备周围外,均涂有指甲油和石蜡。接下来,将它们置于染料中并进行清理,以便观察染料渗透情况。凯塔胶结剂组的微渗漏倾向最小,但各组之间无统计学差异。