Visualization of PEO-PBLA-pyrene polymeric micelles by atomic force microscopy.

作者信息

Liaw J, Aoyagi T, Kataoka K, Sakurai Y, Okano T

机构信息

Department of Pharmaceutics, School of Pharmacy, Taipei Medical College, Taiwan.

出版信息

Pharm Res. 1998 Nov;15(11):1721-6. doi: 10.1023/a:1011908728838.

Abstract

PURPOSE

To directly visualize and evaluate the aqueous block copolymeric micelles, poly(ethylene oxide)-poly(beta-benzyl L-aspartate) (PEO-PBLA) chemically conjugated with pyrene fluorescence molecule, by nanotechnology of atomic force microscopy (AFM).

METHODS

The block copolymers' PEO-PBLA-Pyrene was first synthesized by reacting with pyrene sulfonyl chloride and PEO-PBLA in tetrahydrofuran (THF) solution and were identified by GPC reflect index, UV and fluorescence detectors. The characterization of physical and chemical properties of PEO-PBLA-Pyrene polymeric micellar solution were examined by the dynamic light scattering (DLS) and critical micelles concentrations (CMC). In addition, the nanotechnology of AFM was used to directly visualize the size and shape of nanopolymeric micelles.

RESULTS

The pyrene fluorescence molecule were successfully conjugated at the amino group of the end of PBLA chain by GPC with three different detectors. The size of the aqueous PEO-PBLA-Pyrene polymeric micelles was detected around 57 nm with unimodal distribution by DLS measurement. As a result of this finding, the CMC test was also found out that the fluorescence intensity was increasing around 0.01 approximately 0.05 mg/ml. Using AFM evaluation of polymeric micellar solution, the morphology of aqueous PEO-PBLA-Pyrene polymeric micelles was observed on round shape and with the narrow dispersity of size range 50 approximately 80 nm.

CONCLUSIONS

The presence of PEO-PBLA copolymers with pyrene in an aqueous system formed in a spherical and nano range of polymeric micelles.

摘要

目的

通过原子力显微镜(AFM)纳米技术直接观察和评估与芘荧光分子化学共轭的水性嵌段共聚物胶束聚(环氧乙烷)-聚(β-苄基-L-天冬氨酸)(PEO-PBLA)。

方法

首先通过芘磺酰氯与PEO-PBLA在四氢呋喃(THF)溶液中反应合成嵌段共聚物PEO-PBLA-芘,并通过凝胶渗透色谱(GPC)示差折光指数、紫外和荧光检测器进行鉴定。通过动态光散射(DLS)和临界胶束浓度(CMC)检测PEO-PBLA-芘聚合物胶束溶液的物理和化学性质。此外,利用AFM纳米技术直接观察纳米聚合物胶束的大小和形状。

结果

通过GPC和三种不同的检测器成功地将芘荧光分子共轭在PBLA链末端的氨基上。通过DLS测量,检测到水性PEO-PBLA-芘聚合物胶束的大小约为57nm,呈单峰分布。基于这一发现,CMC测试还发现荧光强度在约0.01至0.05mg/ml左右增加。通过对聚合物胶束溶液的AFM评估,观察到水性PEO-PBLA-芘聚合物胶束的形态为圆形,大小范围在50至80nm之间,分散度较窄。

结论

在水性体系中,PEO-PBLA共聚物与芘形成了球形且纳米级的聚合物胶束。