Abstract

Parietal craniotomies of the mature rabbit skull were repositioned and fixed with resorbable plate and screws made of LactoSorb (Walter Lorenz Surgical, Jacksonville, FL) poly L-lactic acid (PLLA) and polyglycolic acid (PGA) in 20 mature rabbits. Changes in the resorbable devices as well as at the tissue-implant interface were evaluated at 2, 6, 9, and 12 months postoperatively. At 2 months, no change in the size of the implants was seen with a noninflammatory layer of surrounding fibrous tissue and intense birefringence of the screws. At 6 months, substantial loss of implant size had occurred, accompanied by fibrovascular and a macrophage cellular infiltrate. At 9 months, more than 95% of the implant was resorbed, with a small amount remaining in the screw hole. Other than macrophages within the remaining material, very few giant cells were seen. By 1 year, no evidence of birefringent macromolecular polymer debris could be found. No contraindications for the clinical use of this specific PLLA-PGA copolyer could be found when implanted on craniofacial bone surface.

摘要

在20只成年兔中,采用由LactoSorb(佛罗里达州杰克逊维尔市的Walter Lorenz Surgical公司生产)聚L-乳酸(PLLA)和聚乙醇酸(PGA)制成的可吸收板和螺钉,对成年兔颅骨的顶骨开颅部位进行重新定位和固定。在术后2、6、9和12个月评估可吸收装置以及组织-植入物界面的变化。术后2个月,植入物大小未见变化,周围有一层无炎症的纤维组织,螺钉呈现强烈双折射。术后6个月,植入物大小出现显著减小,伴有纤维血管和巨噬细胞浸润。术后9个月,超过95%的植入物被吸收,仅有少量残留在螺钉孔中。除了残留材料中的巨噬细胞外,很少见到巨细胞。到1年时,未发现双折射大分子聚合物碎片的迹象。当将这种特定的PLLA-PGA共聚物植入颅面骨表面时,未发现临床使用的禁忌证。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验