Suppr超能文献

六年后的白榴石增强玻璃陶瓷嵌体:粘结性复合材料的磨损

Leucite-reinforced glass ceramic inlays after six years: wear of luting composites.

作者信息

Krämer N, Frankenberger R

机构信息

Policlinic for Operative Dentistry and Periodontology, University of Erlangen-Nuremberg, Glueckstrasse 11, D-91054 Erlangen, Germany.

出版信息

Oper Dent. 2000 Nov-Dec;25(6):466-72.

Abstract

Wear of luting composites is still an unsolved problem with adhesive inlays. However, only limited clinical research has been conducted regarding this phenomenon. This study evaluated the substance loss within the luting gap over a six-year period in vivo. In the course of a controlled prospective clinical study, 16 patients received 39 Class-II IPS Empress inlays. Variolink Low (Vivadent; n = 18) was used as conventional low-viscosity luting composite, the hybrid-type restorative resin composite Tetric (n = 21; Vivadent) was applied according to the ultrasonic insertion technique. The restorations were clinically assessed after 6, 12, 24, 36, 48 and 72 months and replicas were made. The contact-free occlusal areas of the replicas were scanned by use of a computer-controlled profilometer (Perthen S3P), the analysis of the data was computed using a newly developed software (Xpert for Windows 95) and statistically analyzed with non-parametric tests. After six months all restorations exhibited marginal ditching. The percentage of detectable luting gap abrasion increased between each recall appointment (32% after six months, 48% after 12 months, 46% after 24 months, 55% after 36 months, 59% after 48 months and 65% after 72 months). Except for the 48-months results, no significant difference between the materials used for luting was evident (p > 0.05). Between the width and the depth of the luting space a linear regression was computed. The quantitative evaluation clearly demonstrated that hopes of relevantly reduced wear of luting composites were not confirmed when using the higher filled luting material.

摘要

粘结性嵌体中粘结性复合材料的磨损仍是一个未解决的问题。然而,关于这一现象仅进行了有限的临床研究。本研究评估了体内六年期间粘结间隙内的物质损失。在一项对照前瞻性临床研究过程中,16例患者接受了39颗II类IPS Empress嵌体。Variolink Low(Vivadent;n = 18)用作传统的低粘度粘结性复合材料,混合型修复树脂复合材料Tetric(n = 21;Vivadent)根据超声插入技术应用。在6、12、24、36、48和72个月后对修复体进行临床评估并制作复制件。使用计算机控制的轮廓仪(Perthen S3P)扫描复制件的无接触咬合区域,使用新开发的软件(适用于Windows 95的Xpert)计算数据并进行分析,并用非参数检验进行统计学分析。六个月后,所有修复体均出现边缘沟。每次复诊时可检测到的粘结间隙磨损百分比增加(六个月后为32%,12个月后为48%,24个月后为46%,36个月后为55%,48个月后为59%,72个月后为65%)。除48个月的结果外,所用粘结材料之间无明显差异(p>0.05)。计算了粘结空间的宽度和深度之间的线性回归。定量评估清楚地表明,使用高填充粘结材料时,粘结性复合材料磨损显著降低的希望未得到证实。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验