Suppr超能文献

铒铬:钇-钪-镓石榴石激光制备的II类洞型中复合树脂充填体的微渗漏

Microleakage of composite fillings in Er,Cr:YSGG laser-prepared class II cavities.

作者信息

Gutknecht N, Apel C, Schäfer C, Lampert F

机构信息

Department for Conservative Dentistry, Periodontology, and Preventive Dentistry, University of Aachen, 52074 Aachen, Germany.

出版信息

Lasers Surg Med. 2001;28(4):371-4. doi: 10.1002/lsm.1064.

Abstract

BACKGROUND AND OBJECTIVE

If there is insufficient bonding to the enamel, the shrinkage of composites that occurs during polymerization can result in a gap between the filling material and the cavity wall. This gap permits the passage of bacteria or their metabolic products and also of various molecules and ions. This leads to hypersensitivity or secondary caries and is thus one of the causes of the failures encountered in composite restorations. The aim of this study was to examine the quality of the margins of composite fillings in Er,Cr:YSGG laser-prepared cavities by means of dye penetration. The results were compared with those of restoration in conventionally prepared and conditioned cavities.

STUDY DESIGN/MATERIALS AND METHODS: To this end, 45 class II cavities in extracted molars were prepared. The teeth were divided into three groups. The first group served as a control group. The cavities were prepared in the classical manner by using a diamond, beveled and subsequently conditioned by the etching method. In group 2, the cavities were prepared and conditioned exclusively with the Er,Cr:YSGG laser. In group 3, laser preparation was supplemented by conditioning of the cavity with phosphoric acid.

RESULTS

No significant difference could be found between the classical preparation technique in combination with etching and the laser preparation method with supplementary etching (group 3). The degree of dye penetration was highest in the group undergoing laser-prepared restoration without additional etching (group 2) (Wilcoxon test, P < 0.017).

CONCLUSIONS

Although it was found in previous studies that there is no significant difference between bond strength of acid etched enamel and Er,Cr:YSGG laser etched enamel, the dye penetration rate differs. On the basis of the results of our study, the additional use of etching after Er,Cr:YSGG laser preparation is recommended as it is used in the classical cavity preparation technique.

摘要

背景与目的

如果与牙釉质的粘结不足,聚合过程中复合材料的收缩会导致填充材料与洞壁之间出现间隙。这个间隙会使细菌或其代谢产物以及各种分子和离子通过。这会导致牙齿敏感或继发龋,因此是复合树脂修复失败的原因之一。本研究的目的是通过染料渗透法检查铒铬:钇钪镓石榴石(Er,Cr:YSGG)激光制备的窝洞中复合树脂充填体边缘的质量。将结果与传统制备和预处理窝洞的修复结果进行比较。

研究设计/材料与方法:为此,在拔除的磨牙上制备了45个II类窝洞。将牙齿分为三组。第一组作为对照组。窝洞采用经典方法用金刚石制备,进行斜面制备,随后采用酸蚀法进行预处理。在第2组中,窝洞仅用Er,Cr:YSGG激光制备和预处理。在第3组中,激光制备后用磷酸对窝洞进行补充预处理。

结果

经典制备技术结合酸蚀与激光制备方法并补充酸蚀(第3组)之间未发现显著差异。在未进行额外酸蚀的激光制备修复组(第2组)中染料渗透程度最高(Wilcoxon检验,P < 0.017)。

结论

尽管在先前的研究中发现酸蚀牙釉质和Er,Cr:YSGG激光蚀刻牙釉质的粘结强度没有显著差异,但染料渗透速率不同。根据我们的研究结果,建议在Er,Cr:YSGG激光制备后额外使用酸蚀,就像在经典窝洞制备技术中那样。