Suppr超能文献

正畸镍钛合金丝的腐蚀行为与表面结构

Corrosion behavior and surface structure of orthodontic Ni-Ti alloy wires.

作者信息

Iijima M, Endo K, Ohno H, Yonekura Y, Mizoguchi I

机构信息

Department of Orthodontics, School of Dentistry, Health Sciences University of Hokkaido, Kanazawa 1757, Ishikari-Tobetsu, Hokkaido 061-0293, Japan.

出版信息

Dent Mater J. 2001 Mar;20(1):103-13. doi: 10.4012/dmj.20.103.

Abstract

The corrosion behaviors of a commercial Ni-Ti alloy orthodontic wire and a polished plate with same composition in 0.9% NaCl and 1% lactic acid solutions were examined using an electrochemical technique, an analysis of released ions, and a surface analysis by X-ray photoelectron spectroscopy (XPS). The effect of polishing the wire on the corrosion was also examined. The XPS analysis demonstrated the presence of a thick oxide film mainly composed of TiO2 with trace amounts of Ni hydroxide, which had formed on the wire surface during the heat treatment and subsequent pickling processes. This oxide layer contributed to the higher resistance of the as-received wire to both general and localized corrosion in 0.9% NaCl solution, compared with that of the polished plate and the polished wire. The thick oxide layer, however, was not stable and did not protect the orthodontic wire from corrosion in 0.1% lactic acid solution.

摘要

采用电化学技术、释放离子分析以及X射线光电子能谱(XPS)表面分析等方法,研究了一种商用镍钛合金正畸丝和具有相同成分的抛光板在0.9%氯化钠溶液和1%乳酸溶液中的腐蚀行为。还研究了对正畸丝进行抛光处理对腐蚀的影响。XPS分析表明,在热处理和随后的酸洗过程中,正畸丝表面形成了一层主要由TiO₂组成并含有微量氢氧化镍的厚氧化膜。与抛光板和抛光后的正畸丝相比,该氧化层使原始正畸丝在0.9%氯化钠溶液中对全面腐蚀和局部腐蚀具有更高的抗性。然而,该厚氧化层不稳定,无法保护正畸丝在0.1%乳酸溶液中免受腐蚀。