Angle Orthod. 2018 Jul;88(4):450-457. doi: 10.2319/092917-655.1. Epub 2018 Mar 6.
The aim of this research was to assess galvanic behavior of lingual orthodontic brackets coupled with representative types of orthodontic wires.
Three types of lingual brackets: Incognito (INC), In-Ovation L (IOV), and STb (STB) were combined with a stainless steel (SS) and a nickel-titanium (NiTi) orthodontic archwire. All materials were initially investigated by scanning electron microscopy / x-ray energy dispersive spectroscopy (SEM/EDX) while wires were also tested by x-ray diffraction spectroscopy (XRD). All bracket-wire combinations were immersed in acidic 0.1M NaCl 0.1M lactic acid and neutral NaF 0.3% (wt) electrolyte, and the potential differences were continuously recorded for 48 hours.
The SEM/EDX analysis revealed that INC is a single-unit bracket made of a high gold (Au) alloy while IOV and STB are two-piece appliances in which the base and wing are made of SS alloys. The SS wire demonstrated austenite and martensite iron phase, while NiTi wire illustrated an intense austenite crystallographic structure with limited martensite. All bracket wire combinations showed potential differences below the threshold of galvanic corrosion (200 mV) except for INC and STB coupled with NiTi wire in NaF media.
The electrochemical results indicate that all brackets tested demonstrated galvanic compatibility with SS wire, but fluoride treatment should be used cautiously with NiTi wires coupled with Au and SS brackets.
本研究旨在评估舌侧正畸托槽与代表性类型正畸丝的电偶行为。
将三种类型的舌侧托槽(Incognito[INC]、In-Ovation L[IOV]和 STb[STB])与不锈钢(SS)和镍钛(NiTi)正畸弓丝组合。所有材料均通过扫描电子显微镜/ X 射线能量色散光谱(SEM/EDX)进行初步研究,而弓丝也通过 X 射线衍射光谱(XRD)进行测试。所有托槽-弓丝组合均浸入酸性 0.1M NaCl 0.1M 乳酸和中性 NaF 0.3%(wt)电解质中,并连续记录 48 小时的电位差。
SEM/EDX 分析表明,INC 是一种由高金(Au)合金制成的单单元托槽,而 IOV 和 STB 是由 SS 合金制成的两件式器械,其中底座和翼由 SS 合金制成。SS 丝显示出奥氏体和马氏体铁相,而 NiTi 丝则显示出强烈的奥氏体晶体结构,马氏体相有限。除了在 NaF 介质中与 NiTi 丝结合的 INC 和 STB 之外,所有托槽-弓丝组合的电位差均低于电偶腐蚀的阈值(200 mV)。
电化学结果表明,所有测试的托槽均与 SS 丝表现出电偶相容性,但在 Au 和 SS 托槽与 NiTi 丝结合时应谨慎使用氟化物处理。