Rauschmann Michael A, Wichelhaus Thomas A, Stirnal Volker, Dingeldein Elvira, Zichner Ludwig, Schnettler Reinhard, Alt Volker
Department of Orthopaedic Surgery, University Hospital, Johann-Wolfgang-Goethe-University, Marienburgstrasse 2, 60528 Frankfurt am Main, Germany.
Biomaterials. 2005 May;26(15):2677-84. doi: 10.1016/j.biomaterials.2004.06.045.
The use of polymethylmetacrylate beads for local delivery of antibiotics requires a second surgical procedure for their removal and resorbable calcium sulphate exhibits cytotoxic effects. In this work, a bioresorbable composite of calcium sulphate and nanoparticulate hydroxyapatite (PerOssal was studied regarding its antibiotic release properties and biocompatibility. Material characteristics of plain PerOssal and pure calcium sulphate pellets were studied using scanning and electron microscopy and X-ray methods. Pellets were soaked with gentamicin and vancomycin, respectively. Release properties of both antibiotics from both materials were investigated over 10 days. Quantitative and qualitative cytotoxic assays were performed for biocompatibility testing. Specific surface was 106 m(2)/g for PerOssal and 2.2 m(2)/g for pure calcium sulphate. Almost complete elution of gentamicin was found for both carrier materials (94.7% for PerOssal vs. 95.8% for calcium sulphate) within 10 days, whereas vancomycin release was higher for PerOssal (96.3% vs. 74.8%). PerOssal showed higher initial and lower release after approximately 5 days compared to calcium sulphate. No significant in vitro cytotoxic differences were found between PerOssal and nontoxic cell culture medium. Calcium sulphate showed cytotoxic effects in two out of four tests. PerOssal exhibits excellent properties regarding resorption, biocompatibility, and antibiotic release.
使用聚甲基丙烯酸甲酯珠粒进行抗生素局部递送需要通过第二次外科手术将其取出,且可吸收硫酸钙具有细胞毒性作用。在本研究中,对硫酸钙与纳米羟基磷灰石的生物可吸收复合材料(PerOssal)的抗生素释放特性和生物相容性进行了研究。使用扫描电子显微镜和X射线方法研究了普通PerOssal和纯硫酸钙颗粒的材料特性。颗粒分别用庆大霉素和万古霉素浸泡。研究了两种材料中两种抗生素在10天内的释放特性。进行了定量和定性细胞毒性试验以进行生物相容性测试。PerOssal的比表面积为106 m²/g,纯硫酸钙的比表面积为2.2 m²/g。在10天内,两种载体材料中庆大霉素几乎完全洗脱(PerOssal为94.7%,硫酸钙为95.8%),而PerOssal中万古霉素的释放量更高(96.3%对74.8%)。与硫酸钙相比,PerOssal在大约5天后显示出更高的初始释放量和更低的释放量。PerOssal与无毒细胞培养基之间未发现显著的体外细胞毒性差异。硫酸钙在四项测试中的两项中显示出细胞毒性作用。PerOssal在吸收、生物相容性和抗生素释放方面表现出优异的性能。