Suppr超能文献

两种自酸蚀底漆在3个月储存期内的粘结强度比较。

Bond strength comparison of 2 self-etching primers over a 3-month storage period.

作者信息

Trites Brian, Foley Timothy F, Banting David

机构信息

Division of Graduate Orthodontics, School of Dentistry, University of Western Ontario, London, Ontario, Canada.

出版信息

Am J Orthod Dentofacial Orthop. 2004 Dec;126(6):709-16. doi: 10.1016/j.ajodo.2003.09.032.

Abstract

The purpose of this in vitro study was to evaluate the shear-peel bond strength of 2 self-etching primer systems, Transbond Plus (3M/ Unitek, Monrovia, Calif) and First Step (Reliance Orthodontic Products, Itasca, Ill), with their respective adhesives, and compare them with a control adhesive system (Transbond XT, 3M/ Unitek) over a 3-month period. Two hundred seventy extracted human premolars were obtained and randomly divided into 9 groups of 30 teeth. Metal orthodontic brackets were bonded to the enamel, and each adhesive group was stored for 24 horrs (T1), 30 days (T2), or 3 months (T3) in deionized water at 37 degrees C. All bonded specimens were thermocycled at 10 degrees C and 50 degrees C for 24 hours before debonding. Brackets were debonded by using a shear-peel load on a testing machine at a cross-head speed of 2 mm/min. Bond failure was also evaluated. The shear-peel bond strengths of the 3 bonding systems were clinically acceptable with the possible exception of First Step at 30-day storage. Repeated measures analysis of variance showed a statistically significant (P < .0001) difference in mean bond strengths between the 3 adhesive systems. The shear-peel bond strength of the adhesives over the 3 time intervals showed statistically significant (P = .005) changes. In each group, there were statistically significant differences in shear-peel bond strength between time intervals T1-T2 and T2-T3 for Transbond Plus and T2-T3 for First Step. The change in mean shear-peel bond strength of the 3 adhesives demonstrated a consistent pattern of behavior over the 3 storage intervals. The lowest mean shear-peel bond strength values were noted at the 30-day storage. Bond failure analysis (adhesive remnant index) demonstrated mainly cohesive bond failures.

摘要

本体外研究的目的是评估两种自酸蚀底漆系统(Transbond Plus,3M/Unitek公司,加利福尼亚州蒙罗维亚;First Step,Reliance Orthodontic Products公司,伊利诺伊州伊塔斯卡)与各自的粘合剂之间的剪切-剥离粘结强度,并在3个月的时间内将它们与对照粘合剂系统(Transbond XT,3M/Unitek)进行比较。获取了270颗拔除的人类前磨牙,并随机分为9组,每组30颗牙齿。将金属正畸托槽粘结到牙釉质上,每个粘合剂组在37℃的去离子水中储存24小时(T1)、30天(T2)或3个月(T3)。在脱粘之前,所有粘结标本在10℃和50℃下进行24小时的热循环。使用测试机以2mm/min的十字头速度施加剪切-剥离载荷使托槽脱粘。还评估了粘结失败情况。除了储存30天时的First Step可能例外,这三种粘结系统的剪切-剥离粘结强度在临床上是可接受的。重复测量方差分析显示,三种粘合剂系统之间的平均粘结强度存在统计学上的显著差异(P <.0001)。三种粘合剂在三个时间间隔内的剪切-剥离粘结强度显示出统计学上的显著变化(P =.005)。在每组中,Transbond Plus在T1-T2时间间隔以及First Step在T2-T3时间间隔之间的剪切-剥离粘结强度存在统计学上的显著差异。三种粘合剂的平均剪切-剥离粘结强度变化在三个储存间隔内呈现出一致的行为模式。在储存30天时观察到最低的平均剪切-剥离粘结强度值。粘结失败分析(粘合剂残留指数)主要显示为内聚粘结失败。