Bayani Shahin, Ghassemi Amirreza, Manafi Safa, Delavarian Mohadeseh
Department of Orthodontics, School of Dentistry, Kerman University of Medical Science, Kerman, Iran.
Kerman Oral and Dental Diseases Research Center, Kerman University of Medical Science, Kerman, Iran.
Dent Res J (Isfahan). 2015 May-Jun;12(3):265-70.
The purpose of this study was to evaluate the effect of light-curing time on the shear bond strength (SBS) of two orthodontic color-change adhesives (CCAs).
A total of 72 extracted premolars were randomly assigned into 6 groups of 12 teeth each. Subsequent to primer application, a metal bracket was bonded to the buccal surface using an orthodontic adhesive. Two CCAs (Greengloo and Transbond Plus) were tested and one conventional light-cured adhesive (Resilience) served as control. For each adhesive, the specimens were light-cured for two different times of 20 and 40 s. All the specimens underwent mechanical testing using a universal testing machine to measure the SBS. Adhesive remnant index (ARI) was used to assess the remnant adhesive material on the tooth surface. All statistical analyses were performed using SPSS software. The significance level for all statistical tests was set at P ≤ 0.05.
The SBSs of the tested groups were in the range of 14.05-31.25 MPa. Greengloo adhesive showed the highest SBS values when light-cured for 40 s, and Transbond Plus adhesive showed the lowest values when light-cured for 20 s. ARI scores of Transbond Plus adhesive were significantly higher than those of controls, while other differences in ARI values were not significant.
Within the limitations of his study, decreasing the light-curing time from 40 to 20 s decreased the SBS of the tested adhesives; however, this decline in SBS was statistically significant only in Transbond Plus adhesive.
本研究的目的是评估光固化时间对两种正畸变色粘合剂(CCA)剪切粘结强度(SBS)的影响。
总共72颗拔除的前磨牙被随机分为6组,每组12颗牙齿。在涂抹底漆后,使用正畸粘合剂将金属托槽粘结到颊面。测试了两种CCA(Greengloo和Transbond Plus),并将一种传统的光固化粘合剂(Resilience)作为对照。对于每种粘合剂,样本分别在20秒和40秒这两个不同的时间进行光固化。所有样本使用万能试验机进行力学测试以测量SBS。使用粘结剂残留指数(ARI)来评估牙齿表面的残留粘结材料。所有统计分析均使用SPSS软件进行。所有统计检验的显著性水平设定为P≤0.05。
测试组的SBS在14.05 - 31.25MPa范围内。Greengloo粘合剂在光固化40秒时显示出最高的SBS值,而Transbond Plus粘合剂在光固化20秒时显示出最低的值。Transbond Plus粘合剂的ARI评分显著高于对照组,而ARI值的其他差异不显著。
在本研究的局限性范围内,将光固化时间从40秒减少到20秒会降低测试粘合剂的SBS;然而,这种SBS的下降仅在Transbond Plus粘合剂中具有统计学意义。