Barrios Carlos A, Xu Qingwei, Cutright Teresa, Newby Bi-min Zhang
Department of Chemical Engineering, The University of Akron, Akron, OH 44325-3906, USA.
Colloids Surf B Biointerfaces. 2005 Mar 25;41(2-3):83-93. doi: 10.1016/j.colsurfb.2004.09.009. Epub 2004 Dec 18.
Biofouling has posed serious problems in maritime industry including increased fuel consumptions, economic loss from ship-hull maintenances, contamination of drinking water, and serious corrosion for mechanical instruments. Minimizing the attachment of bacteria and formation of biofilm could be advantageous in reducing the early stages of biofouling. Zosteric acid, a natural product present in eelgrass, was found to have ability for preventing the attachment of some bacteria and barnacles. In this study, the antifouling ability of zosteric acid during the early stages of fouling was evaluated using attachment studies of fresh water bacteria. Simultaneously, various methods were sought for incorporating zosteric acid into silicone to prolong the release of the compound. The main results from this study were that zosteric acid exhibited anti-bacterial attachment regardless of whether it dispersed in water or incorporated into a coating. In addition, the release rate of zosteric acid from the incorporated coatings, particularly those where zosteric acid was uniformly dispersed with aggregates size of 4 microm or less, was orders of magnitude slower than those of previous reports. The release results indicate that the service life of our coatings could be far extended even with a small amount of zosteric acid incorporated.
生物污损给海运业带来了严重问题,包括燃油消耗增加、船体维护造成的经济损失、饮用水污染以及机械设备的严重腐蚀。尽量减少细菌附着和生物膜形成,在减少生物污损的早期阶段可能具有优势。带状酸是一种存在于大叶藻中的天然产物,被发现具有防止某些细菌和藤壶附着的能力。在本研究中,通过淡水细菌附着研究评估了带状酸在污损早期阶段的防污能力。同时,寻求了各种将带状酸掺入硅酮中的方法,以延长该化合物的释放时间。本研究的主要结果是,无论带状酸是分散在水中还是掺入涂层中,它都表现出抗菌附着能力。此外,带状酸从掺入涂层中的释放速率,特别是那些带状酸均匀分散且聚集体尺寸为4微米或更小的涂层,比以前的报告慢几个数量级。释放结果表明,即使掺入少量带状酸,我们涂层的使用寿命也可以大大延长。