Heintze Siegward D, Forjanic Monika
Research & Development, In Vitro Research, Ivoclar Vivadent, Schaan, Liechtenstein.
Oper Dent. 2005 Sep-Oct;30(5):617-26.
This study measured the effect of toothbrushing with a slurry of toothpaste on different dental materials that have been optimally polished. Specimens (n=8) of 21 dental materials, 16 resin composites, 1 amalgam and 4 ceramic materials, were subjected to 36,000 cycles (approximately five hours) of circular toothbrushing with a force of 1.7 N and a slurry of toothpaste (RDA 75) in a device for simulated toothbrushing. The unpolished enamel and dentin of extracted anterior teeth were used as a control. The mean roughness (Ra) was measured with an optical sensor (FRT MicroProf) before and after toothbrushing. To compare the roughness of the different materials, ANOVA with a post hoc Tukey B test was applied (p<0.05). Among the resin composites, the hybrid composites showed the greatest increase in mean roughness, while the microfilled composites and the compomer Compoglass F demonstrated the lowest increase. No statistically significant difference in roughness was found before and after simulated toothbrushing for the Amalcap amalgam, Esthet-X resin composite, TPH Spectrum resin composite, d.SIGN ceramic and the experimental ceramic. The other ceramic materials and dentin and enamel specimens showed a statistically significant decrease in mean roughness after simulated toothbrushing. Glazed Empress demonstrated a statistically significant higher initial roughness than polished Empress. For resin composites, no correlation was found between the mean particle size and mean roughness after simulated toothbrushing.
本研究测量了使用牙膏浆液刷牙对经过最佳抛光的不同牙科材料的影响。对21种牙科材料的样本(n = 8)进行测试,其中包括16种树脂复合材料、1种汞合金和4种陶瓷材料,在模拟刷牙装置中,以1.7 N的力和牙膏浆液(相对磨损率75)对其进行36000次循环(约5小时)的圆周刷牙。将拔除前牙的未抛光牙釉质和牙本质用作对照。在刷牙前后使用光学传感器(FRT MicroProf)测量平均粗糙度(Ra)。为比较不同材料的粗糙度,应用方差分析及事后Tukey B检验(p<0.05)。在树脂复合材料中,混合复合材料的平均粗糙度增加最大,而微填料复合材料和复合体Compoglass F的增加最小。对于Amalcap汞合金、Esthet-X树脂复合材料、TPH Spectrum树脂复合材料、d.SIGN陶瓷和实验陶瓷,模拟刷牙前后粗糙度无统计学显著差异。其他陶瓷材料以及牙本质和牙釉质样本在模拟刷牙后平均粗糙度有统计学显著降低。上釉的Empress显示出比抛光的Empress具有统计学显著更高的初始粗糙度。对于树脂复合材料,模拟刷牙后平均粒径与平均粗糙度之间未发现相关性。