Schiff Nicolas, Boinet Mickaël, Morgon Laurent, Lissac Michèle, Dalard Francis, Grosgogeat Brigitte
L.E.I.B.O, Faculty of Odontology, UCBL, Lyon, France.
Eur J Orthod. 2006 Jun;28(3):298-304. doi: 10.1093/ejo/cji102. Epub 2006 Jan 20.
The aim of this investigation was to determine the influence of fluoride in certain mouthwashes on the risk of corrosion through galvanic coupling of orthodontic wires and brackets. Two titanium alloy wires, nickel-titanium (NiTi) and copper-nickel-titanium (CuNiTi), and the three most commonly used brackets, titanium (Ti), iron-chromium-nickel (FeCrNi) and cobalt-chromium (CoCr), were tested in a reference solution of Fusayama-Meyer artificial saliva and in two commercially available fluoride (250 ppm) mouthwashes, Elmex and Meridol. Corrosion resistance was assessed by inductively coupled plasma-atomic emission spectrometry (ICP-MS), analysis of released metal ions, and a scanning electron microscope (SEM) study of the metal surfaces after immersion of different wire-bracket pairs in the test solutions. The study was completed by an electrochemical analysis. Meridol mouthwash, which contains stannous fluoride, was the solution in which the NiTi wires coupled with the different brackets showed the highest corrosion risk, while in Elmex mouthwash, which contains sodium fluoride, the CuNiTi wires presented the highest corrosion risk. Such corrosion has two consequences: deterioration in mechanical performance of the wire-bracket system, which would negatively affect the final aesthetic result, and the risk of local allergic reactions caused by released Ni ions. The results suggest that mouthwashes should be prescribed according to the orthodontic materials used. A new type of mouthwash for use during orthodontic therapy could be an interesting development in this field.
本研究的目的是确定某些漱口水中的氟化物通过正畸钢丝和托槽的电偶耦合对腐蚀风险的影响。在Fusayama-Meyer人工唾液参考溶液以及两种市售含氟(250 ppm)漱口水(Elmex和Meridol)中,对两种钛合金丝(镍钛(NiTi)和铜镍钛(CuNiTi))以及三种最常用的托槽(钛(Ti)、铁铬镍(FeCrNi)和钴铬(CoCr))进行了测试。通过电感耦合等离子体原子发射光谱法(ICP-MS)、释放金属离子分析以及对不同丝-托槽组合浸入测试溶液后金属表面的扫描电子显微镜(SEM)研究来评估耐腐蚀性。通过电化学分析完成了该研究。含有氟化亚锡的Meridol漱口水是NiTi丝与不同托槽耦合时显示出最高腐蚀风险的溶液,而在含有氟化钠的Elmex漱口中,CuNiTi丝呈现出最高腐蚀风险。这种腐蚀有两个后果:丝-托槽系统机械性能的恶化,这会对最终美学效果产生负面影响,以及由释放的镍离子引起局部过敏反应的风险。结果表明,应根据所使用的正畸材料来开具漱口水处方。一种用于正畸治疗期间的新型漱口水可能是该领域一个有趣的发展方向。