Suppr超能文献

Long-term clinical failure rate of molar tubes bonded with a self-etching primer.

作者信息

Pandis Nikolaos, Christensen Lars, Eliades Theodore

机构信息

Department of Orthodontics, Aristotle University of Thessaloniki, Greece.

出版信息

Angle Orthod. 2005 Nov;75(6):1000-2. doi: 10.1043/0003-3219(2005)75[1000:LCFROM]2.0.CO;2.

Abstract

The purpose of this study was to assess the long-term in vivo failure rate of tubes bonded to first and second molars with a self-etching primer (SEF). A total of 810 molar tubes (414 first molar and 396 second molar) were bonded on 135 patients (56 male, 79 female; mean age 14 years) with the 3M Transbond Plus Self Etching Primer. The first-time failures of the tubes were recorded for a mean period of 26 months (range 23-29 months). Failure rates per jaw (maxilla-mandible), tooth (first and second molar), and quadrant (left, right) were analyzed with the chi(2) at alpha = 0.05 level of significance. Significant differences were found in the failure rate between first and second molars (9.66% vs 20%, respectively) as well as maxillary and mandibular molars (7.5% vs 21%, respectively). The combined, total failure rate for first and second molars was 14.80%. No difference was found between male and female failure rates for the molar tubes. First-molar tubes bonded with an SEF may show failure rates comparable with those reported in the literature for tubes bonded with conventional acid etching.

摘要

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验