Louly A C, Mora A F, Moore B K, Andres C J, Goodacre C J
Department of Prosthodontics, Indiana University School of Dentistry, Indianapolis 46202.
Int J Prosthodont. 1991 Sep-Oct;4(5):425-31.
Infrared soldering was compared to gas-oxygen torch soldering by testing specimens made from each of the following four classes of metal ceramic alloys: gold-platinum-palladium, gold-palladium, palladium-silver, and nickel-chromium-beryllium. There was no significant difference between infrared and torch soldering for the gold-palladium, palladium-silver, and base metal alloy specimens. However, infrared soldering of the gold-platinum-palladium alloy samples produced significantly weaker joints than those produced by torch soldering.
通过对以下四类金属陶瓷合金制成的试样进行测试,将红外焊接与气氧焊炬焊接进行了比较:金 - 铂 - 钯、金 - 钯、钯 - 银和镍 - 铬 - 铍。对于金 - 钯、钯 - 银和贱金属合金试样,红外焊接和焊炬焊接之间没有显著差异。然而,金 - 铂 - 钯合金样品的红外焊接产生的接头明显比焊炬焊接产生的接头弱。