Tyas M J
School of Dental Science, University of Melbourne.
Aust Dent J. 1991 Aug;36(4):298-301. doi: 10.1111/j.1834-7819.1991.tb00726.x.
Eighty Class V non-undercut cervical abrasion lesions were restored using four dentine bonding agents and composite resin. The restorations were examined over a three-year period, and the cumulative loss rate calculated each year. Marginal staining at each year was assessed using a standardized photographic method. The loss rate of restorations increased generally over the three-year period, reaching 30 to 60 per cent for the four products. Marginal staining also increased for all four products over the three-year period.