Stress intensity factor threshold in dental porcelains.

作者信息

Yoshimura Humberto Naoyuki, Cesar Paulo Francisco, Soki Fabiana Naomi, Gonzaga Carla Castiglia

机构信息

Laboratory of Metallurgy and Ceramic Materials, Institute for Technological Research of the State of São Paulo, Sao Paulo, Brazil.

出版信息

J Mater Sci Mater Med. 2008 May;19(5):1945-51. doi: 10.1007/s10856-007-3290-4. Epub 2007 Oct 18.

Abstract

The stress intensity factor threshold (KI0) is related to the stress level at which cracks start to grow stably, causing the weakening of porcelain prostheses during their use. The values of KI0 of seven dental porcelains (with and without reinforcing leucite crystal, KAlSi2O6) stored in air (22 degrees C, 60% relative humidity) and artificial saliva (37 degrees C) were determined by measuring the crack growth velocity of radial cracks generated at the corner of Vickers indentations. The results of KI0 were correlated with the leucite content, fracture toughness (KIc), and chemical composition of the porcelains. It was observed that KI0 increased with the increase of leucite content (only for the leucite-based porcelains) and with the increase of KIc. The increase in Al2O3 content or the decrease in the alkali oxide (K2O and Na2O) content of the material's glassy matrix tended to increase the KI0 values. Storage media (air and saliva) did not significantly affect the KI0 of porcelains tested, indicating that the control parameter of KI0 value was not the water content of the storage media.

摘要

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验