McCabe J F, Kagi S
Department of Prosthodontics, Dental School, University of Newcastle upon Tyne.
Br Dent J. 1991 Oct 19;171(8):246-8. doi: 10.1038/sj.bdj.4807685.
Compressive strength, fatigue limit, hardness and wear factors were determined for two shades of a composite inlay material both with and without post-cure annealing! The effect of the annealing procedure was to cause a small general improvement in properties. This was more noticeable in the Dentin shade of the material than in the Enamel shade. It is doubtful whether the small improvement in properties would have any significant effect on clinical durability.
测定了一种复合嵌体材料两种色泽在有无后固化退火情况下的抗压强度、疲劳极限、硬度和磨损系数!退火工艺的效果是使性能有小幅总体提升。这在材料的牙本质色泽中比在牙釉质色泽中更明显。性能上的小幅提升是否会对临床耐久性产生任何显著影响尚不确定。