Tunç Emine Sen, Sönmez I Sil Saroğlu, Bayrak Sule, Eğilmez Türkan
Department of Pediatric Dentistry, University of Ondokuz Mayis, Samsun, Turkey.
J Endod. 2008 May;34(5):603-5. doi: 10.1016/j.joen.2008.02.026.
The purpose of this study was to evaluate the bond strength of a resin composite and a polyacid modified composite or "compomer" to white mineral trioxide aggregate (WMTA) with two different bonding systems (total-etch one bottle and self-etch one step). Forty specimens of WMTA were prepared and divided into four groups. In group one, Single Bond (3M/ESPE, St Paul, MN) and Z250 (3M/ESPE) were placed over WMTA. In group two, Prompt L-Pop (3M Dental Products, St Paul, MN) and Z250 were applied. In group three, Single Bond was applied with Dyract AP (Dentsply DeTrey, Konstanz, Germany), and, in group four, Prompt L-Pop was applied with Dyract AP. The shear bond strength was measured, and the fractured surfaces were examined. The results of the shear bond strength tests were analyzed by one-way analysis of variance test. The results of this study have suggested that the total-etch one-bottle adhesive system mediated a stronger bond to WMTA for both the resin composite and the compomer investigated. The placement of composite (Z250) and compomer materials (Dyract AP), used with total-etch one-bottle adhesive (Single Bond), over WMTA as final restoration may be appropriate.
本研究的目的是评估树脂复合材料和聚酸改性复合材料(即“复合体”)在两种不同粘结系统(全酸蚀单组分粘结剂和自酸蚀一步法)下与白色三氧化矿物聚合体(WMTA)的粘结强度。制备了40个WMTA样本并分为四组。第一组,将Single Bond(3M/ESPE,圣保罗,明尼苏达州)和Z250(3M/ESPE)置于WMTA上。第二组,应用Prompt L-Pop(3M牙科产品公司,圣保罗,明尼苏达州)和Z250。第三组,将Single Bond与Dyract AP(登士柏德瑞,康斯坦茨,德国)一起使用,第四组,将Prompt L-Pop与Dyract AP一起使用。测量剪切粘结强度,并检查断裂面。通过单向方差分析对剪切粘结强度测试结果进行分析。本研究结果表明,对于所研究的树脂复合材料和复合体,全酸蚀单组分粘结剂系统介导了与WMTA更强的粘结。在WMTA上使用全酸蚀单组分粘结剂(Single Bond)配合复合树脂材料(Z250)和复合体材料(Dyract AP)作为最终修复可能是合适的。