Bylski David, Wedemeyer Christian, Xu Jie, Sterner Thomas, Löer Franz, von Knoch Marius
Department of Orthopaedics, University of Duisburg-Essen, Germany.
J Biomed Mater Res A. 2009 Jun;89(3):707-16. doi: 10.1002/jbm.a.31956.
Particle-induced osteolysis is the most frequent cause of aseptic loosening after total joint replacement. We performed a study to illuminate the effect of ceramic particles with different diameters and concentrations on the mRNA expression of certain key regulators in particle-induced aseptic osteolysis (RANK, RANKL, OPG, and TNF-alpha) in THP-1 macrophage-like cells. Titanium particles were used as a positive control. RNA was analyzed by quantitative RTPCR. Our results demonstrate that alumina ceramic particles, regardless of particle size, caused only slight upregulations of RANK, TNF-alpha, and OPG mRNA, whose levels were significantly lower in comparison with those of titanium particles (p < 0.05). The continuous increasing tendency to time and particle-dependent mRNA expression of all the parameters stimulated by titanium particles was not found after stimulation with ceramic materials. Even after the concentration of ceramic particles was increased, only a mild upregulation of mRNA expression was found. Furthermore, we observed that the bioinert properties of ceramic particles did not change much in diameters ranging from 0.5 to 1.5 microm. At most of the measuring time points, there was no significant difference between the reactions of the large and small particles in this range. Our results support the theory about the relative bioinert properties of alumina ceramic particles.
颗粒诱导的骨溶解是全关节置换术后无菌性松动最常见的原因。我们进行了一项研究,以阐明不同直径和浓度的陶瓷颗粒对THP-1巨噬细胞样细胞中颗粒诱导的无菌性骨溶解(RANK、RANKL、OPG和TNF-α)某些关键调节因子mRNA表达的影响。钛颗粒用作阳性对照。通过定量RTPCR分析RNA。我们的结果表明,氧化铝陶瓷颗粒,无论粒径大小,仅引起RANK、TNF-α和OPG mRNA的轻微上调,与钛颗粒相比,其水平显著较低(p<0.05)。在用陶瓷材料刺激后,未发现钛颗粒刺激的所有参数的mRNA表达随时间和颗粒依赖性的持续增加趋势。即使陶瓷颗粒浓度增加,也仅发现mRNA表达有轻度上调。此外,我们观察到,直径在0.5至1.5微米范围内的陶瓷颗粒的生物惰性特性变化不大。在大多数测量时间点,该范围内大颗粒和小颗粒的反应之间没有显著差异。我们的结果支持了关于氧化铝陶瓷颗粒相对生物惰性特性的理论。