In the present contribution, electrospinning (e-spinning) was used to fabricate ultra-fine fibers of silk fibroin (SF) from cocoons of indigenous Thai silkworms (Nang-Lai) and Chinese/Japanese hybrid silkworms (DOAE-7). The effects of solution concentration (i.e., 10-40% (w/v) in 85% (v/v) formic acid) and applied electrostatic field strength (EFS; 10, 15 and 20 kV/10 cm) on morphology and size of the electrospun (e-spun) SF products were investigated by scanning electron microscopy. The average diameter of the resulting e-spun SF fibers was found to increase with an increase in both the solution concentration and the EFS value. Specifically, the average diameter of the e-spun SF fibers from Nang-Lai SF solutions ranged between 217 and 610 nm, while that of the fibers from DOAE-7 SF solutions ranged between 183 and 810 nm. The potential for use of the e-spun SF fiber mats as bone scaffolds was assessed with mouse osteoblast-like cells (MC3T3-E1) in which the cells appeared to adhere and proliferate well on their surface.
在本研究中,采用静电纺丝技术(e - 纺丝)从泰国本土蚕(南莱)和中国/日本杂交蚕(DOAE - 7)的茧中制备丝素蛋白(SF)超细纤维。通过扫描电子显微镜研究了溶液浓度(即85%(v/v)甲酸中10 - 40%(w/v))和施加的静电场强度(EFS;10、15和20 kV/10 cm)对静电纺丝(e - 纺)SF产品形态和尺寸的影响。结果发现,所得e - 纺SF纤维的平均直径随溶液浓度和EFS值的增加而增大。具体而言,来自南莱SF溶液的e - 纺SF纤维平均直径在217至610 nm之间,而来自DOAE - 7 SF溶液的纤维平均直径在183至810 nm之间。用小鼠成骨样细胞(MC3T3 - E1)评估了e - 纺SF纤维垫作为骨支架的潜力,结果显示细胞在其表面似乎能很好地黏附并增殖。