Brackett William W, Tay Franklin R, Looney Stephen W, Ito Shuichi, Haisch Larry D, Pashley David H
Department of Oral Rehabilitation, School of Dentistry, Medical College of Georgia, Augusta, USA.
Oper Dent. 2008 May-Jun;33(3):282-6. doi: 10.2341/07-80.
In this study, the microtensile bond strengths of an etch-and-rinse resin adhesive to dentin and enamel and a resin-modified glass ionomer adhesive to dentin were determined on teeth known to have originated from subjects over 60 years of age. The same tests were repeated on teeth originating from young subjects. The resin adhesive was Prime & Bond NT (Caulk/Dentsply), while the resin-modified glass ionomer adhesive was Fuji Bond LC (GC America). Both were paired with the same hybrid resin composite, TPH3 (Caulk/Dentsply). Testing was performed after 48 hours using a "non-trimming" microtensile test at a crosshead speed of 0.6 mm/minute. No significant differences were observed between the young and aged teeth for any comparison (p > 0.05). SEM evaluation of the etched dentinal surfaces demonstrated less depth of decalcification in the intertubular areas of aged dentin, but there was no observable difference within the tubules of young and aged dentin.
在本研究中,在已知来自60岁以上受试者的牙齿上,测定了一种酸蚀冲洗型树脂粘结剂与牙本质和釉质之间以及一种树脂改性玻璃离子粘结剂与牙本质之间的微拉伸粘结强度。对来自年轻受试者的牙齿重复进行相同测试。树脂粘结剂为Prime & Bond NT(Caulk/Dentsply),而树脂改性玻璃离子粘结剂为Fuji Bond LC(GC America)。两者均与相同的复合树脂材料TPH3(Caulk/Dentsply)配对使用。在48小时后,以0.6毫米/分钟的十字头速度采用“不修整”微拉伸试验进行测试。在任何比较中,年轻牙齿和老年牙齿之间均未观察到显著差异(p>0.05)。对酸蚀牙本质表面的扫描电子显微镜评估显示,老年牙本质管间区域的脱钙深度较小,但年轻和老年牙本质小管内未观察到明显差异。