This study determined the bond strengths to Er:YAG laser-irradiated and non-irradiated bovine enamel of three one-step self-etch adhesives (AQ Bond Plus (AQP), G-Bond (GB), and Clearfil Tri-S Bond (TS)) and one two-step self-etch adhesive (Clearfil Megabond (MB)). Eighty SiC paper-ground bovine enamel surfaces were used, of which half were laser-irradiated. The enamel surfaces were bonded to a resin composite with each adhesive, and tensile bond strengths were determined after 24 hours. For non-irradiated enamel groups, MB achieved greater bond strength to enamel than GB and TS (p < 0.05), but no significant difference was found between MB and AQP (p > 0.05). For laser-irradiated enamel groups, no significant differences were found among the four adhesives (p > 0.05). Additionally, for each adhesive, no significant differences were found between laser-irradiated and non-irradiated enamel. It was thus concluded that Er: YAG laser irradiation of enamel did not affect the tensile bond strength of one-step and two-step self-etch adhesives.
本研究测定了三种一步法自酸蚀粘结剂(AQ Bond Plus(AQP)、G-Bond(GB)和Clearfil Tri-S Bond(TS))以及一种两步法自酸蚀粘结剂(Clearfil Megabond(MB))与经铒钇铝石榴石(Er:YAG)激光照射和未照射的牛牙釉质之间的粘结强度。使用了80个经碳化硅砂纸打磨的牛牙釉质表面,其中一半进行了激光照射。用每种粘结剂将牙釉质表面与树脂复合材料粘结,24小时后测定拉伸粘结强度。对于未照射牙釉质组,MB与牙釉质的粘结强度高于GB和TS(p < 0.05),但MB与AQP之间未发现显著差异(p > 0.05)。对于激光照射牙釉质组,四种粘结剂之间未发现显著差异(p > 0.05)。此外,对于每种粘结剂,激光照射和未照射的牙釉质之间未发现显著差异。因此得出结论,牙釉质的Er:YAG激光照射不影响一步法和两步法自酸蚀粘结剂的拉伸粘结强度。