Komori Paula C P, Pashley David H, Tjäderhane Leo, Breschi Lorenzo, Mazzoni Annalisa, de Goes Mario Fernando, Wang Linda, Carrilho Marcela R
Department of Restorative Dentistry, Dental Materials, Piracicaba School of Dentistry, University of Campinas, Brazil.
Oper Dent. 2009 Mar-Apr;34(2):157-65. doi: 10.2341/08-55.
This study evaluated the effect of 2% chlorhexidine digluconate (CHX) used as a therapeutic primer on the long-term bond strengths of two etch-and-rinse adhesives to normal (ND) and caries-affected (CAD) dentin. Forty extracted human molars with coronal carious lesions, surrounded by normal dentin, were selected for this study. The flat surfaces of two types of dentin (ND and CAD) were prepared with a water-cooled high-speed diamond disc, then acid-etched, rinsed and air-dried. In the control groups, the dentin was re-hydrated with distilled water, blot-dried and bonded with a three-step (Scotchbond Multi-Purpose-MP) or two-step (Single Bond 2-SB) etch-and-rinse adhesive. In the experimental groups, the dentin was rehydrated with 2% CHX (60 seconds), blot-dried and bonded with the same adhesives. Resin composite build-ups were made. The specimens were prepared for microtensile bond testing in accordance with the non-trimming technique, then tested either immediately or after six-months storage in artificial saliva. The data were analyzed by ANOVA/Bonferroni tests (alpha = 0.05). CHX did not affect the immediate bond strength to ND or CAD (p > 0.05). CHX treatment significantly lowered the loss of bond strength after six months as seen in the control bonds for ND (p < 0.05), but it did not alter the bond strength of CAD (p > 0.05). The application of MP on CHX-treated ND or CAD produced bonds that did not change over six months of storage.
本研究评估了2%葡萄糖酸氯己定(CHX)作为治疗性底涂剂对两种酸蚀冲洗粘结剂与正常牙本质(ND)和龋损牙本质(CAD)长期粘结强度的影响。本研究选取了40颗拔除的有冠部龋损且周围为正常牙本质的人类磨牙。用带水冷装置的高速金刚石盘制备两种类型牙本质(ND和CAD)的平面,然后进行酸蚀、冲洗和吹干。在对照组中,牙本质用蒸馏水再水化,吸干水分后用三步法(Scotchbond多用途-MP)或两步法(Single Bond 2-SB)酸蚀冲洗粘结剂粘结。在实验组中,牙本质用2% CHX再水化(60秒),吸干水分后用相同的粘结剂粘结。制作树脂复合体修复体。按照非修整技术制备微拉伸粘结测试标本,然后立即测试或在人工唾液中储存6个月后测试。数据通过方差分析/邦费罗尼检验进行分析(α = 0.05)。CHX对与ND或CAD的即时粘结强度没有影响(p > 0.05)。CHX处理显著降低了6个月后ND对照组粘结强度的损失(p < 0.05),但未改变CAD的粘结强度(p > 0.05)。在CHX处理的ND或CAD上应用MP产生的粘结在储存6个月期间没有变化。