Department of Operative Dentistry and Periodontology, University of Freiburg, Freiburg, Germany.
Clin Oral Investig. 2011 Oct;15(5):673-80. doi: 10.1007/s00784-010-0439-1. Epub 2010 Jul 10.
The aim of the study was to investigate changes in the micromorphologyl and microhardness of the enamel surface after bleaching with two different concentrations of hydrogen peroxide (HP) and carbamide peroxide (CP). Bovine enamel samples were embedded in resin blocks, and polished. Specimens in the experimental groups (n = 10) were treated with bleaching gels containing 10% CP, 35% CP, 3.6% HP, and 10% HP, respectively, for 2 h every second day over a period of 2 weeks. The gels had the identical composition and pH and differed only in their HP or CP content. The roughness and morphology of the enamel surface were analyzed using laser profilometry and SEM. Microhardness was measured using a Knoop hardness tester. The data were evaluated statistically. Specimens in the 10% HP group showed significantly higher roughness after bleaching compared to the control group (ΔRa, p = 0.01). Bleaching with 35% CP showed only a tendency to increase roughness (ΔRa, p = 0.06). Application of 10% CP or 3.6% HP had no significant influence on Ra. Enamel microhardness was significantly higher after application of 10% HP compared to the control (ΔMic = 8 KHN, p = 0.0002) and 35% CP (ΔMic = 20KHN, p = 0.01) groups. In summary, application of CP and HP showed only small quantitative and qualitative differences. In addition, the influence of bleaching procedure on the morphology and hardness of the enamel surface depended on the concentration of the active ingredients.
本研究旨在探讨两种不同浓度的过氧化氢(HP)和过氧化脲(CP)漂白后牙釉质微观形貌和显微硬度的变化。牛牙釉质样本被嵌入树脂块中并进行抛光。实验组(n=10)的标本分别用含有 10%CP、35%CP、3.6%HP 和 10%HP 的漂白凝胶处理,每两天处理一次,每次 2 小时,持续 2 周。这些凝胶具有相同的成分和 pH 值,仅在 HP 或 CP 含量上有所不同。使用激光轮廓仪和 SEM 分析牙釉质表面的粗糙度和形貌。使用 Knoop 硬度计测量显微硬度。对数据进行了统计学评估。与对照组相比,10%HP 组的标本在漂白后显示出明显更高的粗糙度(ΔRa,p=0.01)。用 35%CP 漂白仅显示出增加粗糙度的趋势(ΔRa,p=0.06)。应用 10%CP 或 3.6%HP 对 Ra 没有显著影响。与对照组(ΔMic=8KHN,p=0.0002)和 35%CP 组(ΔMic=20KHN,p=0.01)相比,应用 10%HP 后牙釉质的显微硬度显著提高。总之,CP 和 HP 的应用仅显示出微小的定量和定性差异。此外,漂白程序对牙釉质表面形态和硬度的影响取决于活性成分的浓度。