Department of Restorative Dentistry, Dental Research Center São Leopoldo Mandic, Campinas, SP, Brazil.
J Appl Oral Sci. 2009 Nov-Dec;17(6):611-6. doi: 10.1590/s1678-77572009000600014.
The purpose of this study was to assess the effect of home-use bleaching agents containing 10% carbamide peroxide and 7.5% hydrogen peroxide on enamel microhardness and surface micromorphology.
Enamel slabs (n=10) received the bleaching agents for 1 h/day and remained in artificial saliva solution for 23 h/day, during a total period of 21 days. Control group was composed of enamel slabs that were not subjected to treatment with the agents and were maintained in artificial saliva solution. Microhardness tests were performed before treatment application, 21 days of treatment and 14 days after the end of treatment. Scanning electron microscopy analyses were performed after 14 days after the end of bleaching treatment by 3 calibrated observers who attributed scores.
The Tukey's test (alpha=0.05) showed no significant differences in microhardness values among bleaching agents, at 21 days of treatment and a significant increase in microhardness for different agents after 14 days from the end of treatment. Fisher's exact test showed differences in micromorphology of enamel between control and experimental groups (p=0.0342).
Bleaching agents containing 10% carbamide peroxide and 7.5% hydrogen peroxide may change surface micromorphology of enamel, although no changes in microhardness were observed.
本研究旨在评估含有 10%过氧化脲和 7.5%过氧化氢的家用漂白剂对牙釉质显微硬度和表面微观形貌的影响。
将牙釉质样本(n=10)置于漂白剂中,每天使用 1 小时,每天剩余 23 小时置于人工唾液溶液中,共 21 天。对照组由未用药物处理的牙釉质样本组成,并保持在人工唾液溶液中。在治疗前、治疗 21 天后和治疗结束后 14 天进行显微硬度测试。在漂白治疗结束后 14 天,由 3 名经过校准的观察者进行扫描电子显微镜分析,并进行评分。
在治疗 21 天后,Tukey 检验(alpha=0.05)显示不同漂白剂之间的显微硬度值无显著差异,且在治疗结束后 14 天,不同药物的显微硬度显著增加。Fisher 精确检验显示对照组和实验组之间牙釉质微观形态存在差异(p=0.0342)。
含有 10%过氧化脲和 7.5%过氧化氢的漂白剂可能会改变牙釉质的表面微观形貌,尽管在显微硬度方面没有观察到变化。