新型传统不锈钢、回收和无镍正畸托槽的镍释放:体外研究。

Nickel release from new conventional stainless steel, recycled, and nickel-free orthodontic brackets: An in vitro study.

机构信息

Department of Orthodontics, University of Pavia, Italy.

出版信息

Am J Orthod Dentofacial Orthop. 2010 Jun;137(6):809-15. doi: 10.1016/j.ajodo.2008.07.021.

Abstract

INTRODUCTION

The aim of this study was to compare the nickel released from 3 kinds of orthodontic brackets: new conventional stainless steel, recycled stainless steel, and nickel-free brackets.

METHODS

This in-vitro study was performed by using a classic batch procedure. Samples were immersed in artificial saliva at various acidities (pH 4.2, 6.5, 7.6) over an extended time interval (0.25, 1, 24, 48, and 120 hours). The amount of nickel released was determined by using an atomic absorption spectrophotometer and an inductively coupled plasma atomic emission spectrometer. Statistical analysis included a linear regression model for repeated measures, with calculation of Huber White robust standard errors to account for intrabracket correlation of data. For post-hoc comparisons, the Bonferroni correction was applied.

RESULTS

The recycled brackets released the most nickel (74.02 +/- 170.29 microg per gram); the new stainless steel brackets released 7.14 +/- 20.83 microg per gram. The nickel-free brackets released the least nickel (0.03 +/- 0.06 microg per gram). All the differences among the groups were statistically significant (P = 0.000).

CONCLUSIONS

Reconditioned brackets released the most nickel. Moreover, the highest nickel release was recorded in the 2 experiments performed at pH 4.2; it was lower at pH 6.5 and 7.6. Conversely, no relevant differences were observed overall between the maxillary and mandibular arches.

摘要

简介

本研究旨在比较 3 种正畸托槽的镍释放量:新型传统不锈钢、回收不锈钢和无镍托槽。

方法

本体外研究采用经典批量程序进行。将样本在不同酸度(pH 值 4.2、6.5、7.6)的人工唾液中浸泡不同时间(0.25、1、24、48 和 120 小时)。通过原子吸收分光光度计和电感耦合等离子体原子发射光谱仪测定释放的镍量。统计分析包括重复测量的线性回归模型,并计算胡伯怀特稳健标准误差以考虑数据的托槽内相关性。对于事后比较,应用了 Bonferroni 校正。

结果

回收托槽释放的镍最多(每克 74.02 ± 170.29 微克);新型不锈钢托槽释放的镍为每克 7.14 ± 20.83 微克。无镍托槽释放的镍最少(每克 0.03 ± 0.06 微克)。所有组间差异均具有统计学意义(P = 0.000)。

结论

再处理托槽释放的镍最多。此外,在 pH 值为 4.2 的 2 项实验中记录到的镍释放量最高;在 pH 值为 6.5 和 7.6 时较低。相反,在上颌和下颌弓之间总体上未观察到明显差异。