UCL Eastman Dental Institute, Prosthodontics, 256 Gray's Inn Road, London WC1X 8LD, UK.
Dent Mater. 2011 Mar;27(3):253-8. doi: 10.1016/j.dental.2010.10.010. Epub 2010 Nov 13.
To assess the dimensional stability of 8 impression materials over 12 weeks relevant to in vitro tribology studies.
Ten impressions from eight impression materials were taken of a metal block (ADA block) conforming to the American Dental Association specification for impression materials and of another metal block (custom block) which allowed measurements over a larger surface area. The impressions and blocks were scanned on a non-contacting laser profilometer (Taicaan® - Southampton, UK) and using surface metrology software Boddies® (Taicaan® - Southampton, UK) measurements were made at 24h, 2, 4, 8 and 12 weeks. The impression materials tested were [1] Aquasil®, [2] Aquasil® DECA, [3] Affinis®, [4] Express®, [5] Extrude®, [6] Impregum®, [7] President® and [8] Take 1®.
Seven addition silicones and one polyether [6] were tested. [2] and [6] were monophasic, the rest were putty-wash. The results from impressions of the ADA block showed that all materials contracted compared to measurements obtained directly from the block [1] expanded over time (+31.5 μm) (p<0.05). The results from the custom block showed that all materials contracted compared to direct measurements of the block. [4] and [7] expanded over time (+62 μm and +63.8 μm respectively). [8] contracted over time (-54.7 μm) (p<0.05).
No material showed linear changes >1.5% and were stable for 12 weeks. Nevertheless, the range of changes would affect tribology studies were cut-offs lesser than the reported changes are selected. All impressions should be processed after similar time delays to reduce the errors introduced by dimensional changes.
评估 8 种印模材料在体外摩擦学研究相关的 12 周内的尺寸稳定性。
从符合美国牙科协会印模材料规格的金属块(ADA 块)和允许更大表面积测量的另一个金属块(定制块)上各取 8 种印模材料的 10 个印模。使用非接触式激光轮廓仪(英国南安普顿的 Taicaan®)和表面计量软件 Boddies®(英国南安普顿的 Taicaan®)对印模和块进行扫描,在 24h、2、4、8 和 12 周时进行测量。测试的印模材料有 [1]Aquasil®、[2]Aquasil® DECA、[3]Affinis®、[4]Express®、[5]Extrude®、[6]Impregum®、[7]President®和[8]Take 1®。
测试了 7 种加成硅酮和 1 种聚醚[6]。[2]和[6]为单相,其余为糊剂-液体型。ADA 块印模的结果表明,与从块上直接获得的测量值相比,所有材料都收缩[1]随时间膨胀(+31.5μm)(p<0.05)。定制块的结果表明,与块的直接测量值相比,所有材料都收缩。[4]和[7]随时间膨胀(分别为+62μm和+63.8μm)。[8]随时间收缩(-54.7μm)(p<0.05)。
没有一种材料的线性变化超过 1.5%,并且在 12 周内保持稳定。然而,如果选择比报告的变化小的截止值,那么变化范围会影响摩擦学研究。所有印模都应该在类似的时间延迟后进行处理,以减少尺寸变化引入的误差。