Department of Restorative Dentistry, Dental Materials, Piracicaba School of Dentistry, University of Campinas, Piracicaba, SP, Brazil.
Oper Dent. 2010 Nov-Dec;35(6):610-7. doi: 10.2341/09-202-L.
Potassium oxalate desensitizers were previously shown to effectively reduce the immediate permeability of resin-bonded dentin. The current study evaluated whether the effect of the combined application of oxalate with etch-and-rinse adhesives interferes with the durability of resin-dentin bonds when using etch-and-rinse adhesives. The bond strength of resin-bonded dentin specimens composed of two-step or three-step etch-and-rinse adhesives (Single Bond, One-Step and Scotchbond Multi-Purpose, respectively) was tested immediately (24 hours) and after 12 months of water storage. The adhesives were used either according to the manufacturers' instructions (control groups) or after treating acid-etched dentin with a potassium oxalate gel (BisBlock, BISCO, Inc). The treatment of dentin with potassium oxalate was shown to negatively affect the baseline bond strength of resin-bonded dentin specimens, regardless of the adhesive used (p < 0.05). After storage, the bond strength of the resin-bonded interfaces was significantly reduced for all the tested groups (p < 0.001). Nevertheless, the rate of decreasing bond strength was significantly lower for oxalate-treated specimens than for the controls (p < 0.05).
草酸钾脱敏剂先前已被证明能有效地降低树脂粘结牙本质的即刻通透性。本研究评估了草酸与酸蚀-冲洗粘结剂联合应用对使用酸蚀-冲洗粘结剂时树脂-牙本质粘结耐久性的影响。采用两步法或三步法酸蚀-冲洗粘结剂(分别为Single Bond、One-Step 和 Scotchbond Multi-Purpose)制备的树脂粘结牙本质试件的粘结强度在即刻(24 小时)和 12 个月水储存后进行测试。粘结剂根据制造商的说明(对照组)或在用草酸钾凝胶(BisBlock,BISCO,Inc.)处理酸蚀牙本质后使用(处理组)。用草酸钾处理牙本质会降低树脂粘结牙本质试件的基线粘结强度,无论使用哪种粘结剂(p<0.05)。储存后,所有测试组的树脂粘结界面的粘结强度均显著降低(p<0.001)。然而,与对照组相比,处理组的粘结强度下降速度明显较慢(p<0.05)。