University of Sao Paulo, Sao Paulo, Brazil.
Oper Dent. 2012 Jul-Aug;37(4):356-62. doi: 10.2341/09-228-L. Epub 2012 Feb 15.
The objective of this study was to determine whether the hardness of etch-and-rinse adhesives may be affected by the pretreatment of acid-etched dentin with potassium oxalate desensitizer. Unerupted human third molars were cut into crown segments by removing the occlusal enamel and roots. The pulp chamber of these crown segments was connected to a syringe barrel filled with phosphate-buffered saline so that the moisture of dentin was maintained during the bonding procedures. Three etch-and-rinse adhesives-two two-step systems (Adper Single Bond 2 [SB], One-Step [OS]) and one three-step system (Adper Scotchbond Multi-Purpose [MP])-were applied to acid-etched dentin that had been treated (experimental groups) or not (control groups) with potassium oxalate (BisBlock). The Knoop hardness (KHN) of adhesives was taken at different sites of the outer surface of the adhesive-bonded dentin. The KHN of the three tested adhesives applied to acid-etched dentin treated with potassium oxalate was significantly lower than that exhibited by the respective controls (not treated with oxalate; p<0.05). Regardless of the adhesive, the treatment with potassium oxalate reduced the adhesives' KHN (p<0.05), with the OS system exhibiting the lowest KHN compared with the MP and SB systems.
本研究旨在确定草酸钾脱敏剂预处理酸蚀牙本质是否会影响牙本质的硬度。将未萌出的第三磨牙通过去除咬合面釉质和根部分为牙冠段。这些牙冠段的牙髓腔与装满磷酸盐缓冲盐水的注射器筒相连,以使牙本质的水分在粘结过程中得到保持。三种润洗型粘结剂——两种两步法系统(Adper Single Bond 2 [SB],One-Step [OS])和一种三步法系统(Adper Scotchbond Multi-Purpose [MP])——被应用于经过(实验组)或未经(对照组)草酸钾(BisBlock)处理的酸蚀牙本质。在粘结牙本质外表面的不同部位测量粘结剂的努氏硬度(KHN)。应用于经草酸钾处理的酸蚀牙本质的三种测试粘结剂的 KHN 明显低于各自的对照组(未用草酸处理;p<0.05)。无论粘结剂如何,用草酸钾处理都会降低粘结剂的 KHN(p<0.05),与 MP 和 SB 系统相比,OS 系统的 KHN 最低。