ZnSO(3) microrods with uniform size and shape can be prepared under microwave irradiation at much higher speed than a conventional heating bath, usually in minutes. The annealing of ZnSO(3) microrods produced porous ZnO microrods with pore size between 50-200 nm.
ZnSO(3) 微米棒在微波辐射下可以以比传统加热浴更快的速度合成,通常只需几分钟即可完成。ZnSO(3) 微米棒的退火处理得到了具有 50-200nm 孔径的多孔 ZnO 微米棒。