Ricci Hérica Adad, Sanabe Mariane Emi, Costa Carlos Alberto de Souza, Hebling Josimeri
Department of Orthodontics and Pediatric Dentistry, Araraquara School of Dentistry, UNESP--Univ. Estadual Paulista, Araraquara, SP, Brazil.
J Clin Pediatr Dent. 2010 Winter;35(2):163-8. doi: 10.17796/jcpd.35.2.958893530534m503.
The purpose of this study was to compare the immediate microtensile bond strength (microTBS) of two-step etch-and-rinse adhesive systems to the dentin of primary and permanent teeth.
Non-carious human teeth (12 primary molars and 12 premolars) were assigned to 3 groups according to the adhesive system. The adhesive systems were applied to flat superficial coronal dentin surfaces etched with phosphoric acid and composite resin blocks were built up. The teeth were sectioned to produce beam-shaped specimens with 0.81 mm2 cross-sectional area subjected to microTBS testing. MicroTBS data were analyzed statistically by ANOVA and Tukey's test (a = 0.05).
The adhesive systems produced statistically similar mean microTBS to each other (p > 0.05) and no significant differences (p > 0.05) were found when the same material was applied to primary or permanent tooth dentin. The mean microTBS values (MPa) obtained were: Prime & Bond NT: 41.7 +/- 14.4 (permanent) and 40.8 +/- 13.4 (primary); Single Bond: 42.9 +/- 8.6 (permanent) and 41.4 +/- 11.9 (primary); Excite DSC: 46.3 +/- 11.3 (permanent teeth) and 43.4 +/- 12.0 (primary).
There was no difference in the immediate microTBS of two-step etch-and-rinse adhesive systems when applied to the dentin of primary and permanent teeth.
本研究旨在比较两种两步酸蚀冲洗粘结系统与乳牙和恒牙牙本质之间的即刻微拉伸粘结强度(microTBS)。
将无龋坏的人牙(12颗乳牙磨牙和12颗前磨牙)根据粘结系统分为3组。将粘结系统应用于用磷酸蚀刻的平坦冠面表层牙本质表面,并构建复合树脂块。将牙齿切片制成横截面面积为0.81平方毫米的梁形标本,进行微拉伸粘结强度测试。微拉伸粘结强度数据采用方差分析和Tukey检验进行统计学分析(α = 0.05)。
粘结系统之间产生的平均微拉伸粘结强度在统计学上彼此相似(p > 0.05),并且当相同材料应用于乳牙或恒牙牙本质时未发现显著差异(p > 0.05)。获得的平均微拉伸粘结强度值(MPa)为:Prime & Bond NT:恒牙为41.7 +/- 14.4,乳牙为40.8 +/- 13.4;Single Bond:恒牙为42.9 +/- 8.6,乳牙为41.4 +/- 11.9;Excite DSC:恒牙为46.3 +/- 11.3,乳牙为43.4 +/- 12.0。
当应用于乳牙和恒牙牙本质时,两步酸蚀冲洗粘结系统的即刻微拉伸粘结强度没有差异。