Milani Shabnam, Seraj Bahman, Khoshlafz Zahra, Abazarian Niusha
Department of Pediatric Dentistry, School of Dentistry, Tehran University of Medical Sciences, Tehran, Iran.
Private Practice, Hamadan, Iran.
Front Dent. 2020 Sep;17(23):1-7. doi: 10.18502/fid.v17i23.4413. Epub 2020 Sep 25.
Achieving durable restorations with adequate strength in severely damaged primary anterior teeth in children is a priority. The aim of this study was to investigate the effect of dentin pretreatment with chlorhexidine on push-out bond strength of composite restorations.
In this in vitro experimental study, 56 extracted primary anterior teeth were randomly divided into 4 groups: (1) saline and total-etch bonding agent, (2) chlorhexidine and total-etch bonding agent, (3) saline and self-etch bonding agent, and (4) chlorhexidine and self-etch bonding agent. After the application of bonding agents, the post space was filled with Z250 composite resin. Following thermocycling of the samples, the push-out test was performed using a universal testing machine, and the results were analyzed with two-way ANOVA.
The mean push-out bond strength values in groups 1 to 4 were 5.7, 8.39, 5.35, and 7 MPa, respectively. Chlorhexidine groups had significant differences with saline groups in bond strength (P<0.05) but there was no statistically significant difference between the self-etch and total-etch bonding agents in the groups (P>0.05).
Both types of bonding agents (self-etch and total-etch) exhibited favorable results in radicular dentin of primary anterior teeth; however, pre-treatment with chlorhexidine increased the push-out bond strength of composite restorations in primary anterior teeth.
在儿童严重受损的乳前牙中实现具有足够强度的持久修复是首要任务。本研究的目的是调查洗必泰预处理牙本质对复合树脂修复体推出粘结强度的影响。
在这项体外实验研究中,56颗拔除的乳前牙被随机分为4组:(1)生理盐水和全酸蚀粘结剂;(2)洗必泰和全酸蚀粘结剂;(3)生理盐水和自酸蚀粘结剂;(4)洗必泰和自酸蚀粘结剂。应用粘结剂后,桩道用Z250复合树脂充填。对样本进行热循环后,使用万能试验机进行推出试验,结果用双向方差分析进行分析。
第1至4组的平均推出粘结强度值分别为5.7、8.39、5.35和7MPa。洗必泰组与生理盐水组在粘结强度上有显著差异(P<0.05),但各组中自酸蚀粘结剂和全酸蚀粘结剂之间无统计学显著差异(P>0.05)。
两种粘结剂(自酸蚀和全酸蚀)在乳前牙的根管牙本质中均显示出良好的效果;然而,洗必泰预处理提高了乳前牙复合树脂修复体的推出粘结强度。