Abstract

PURPOSE

To evaluate polyalkylimide as a possible vitreous tamponading agent.

METHODS

A 20-gauge pars plana vitrectomy and posterior vitreous detachment were performed in the right eye of six pigmented rabbits. Approximately 1 ml of viscoelastic gel, polyalkylimide (Bio-Alcamid) was thereafter injected into the vitreous space. Full-field ERG and intraocular pressure (IOP, Tonopen) was measured pre-and postoperatively at regular intervals up to 28 days. At day 6 or 28, the rabbits were sacrificed and the eyes were examined macroscopically, photographed, and prepared for histological examination with routine microscopy.

RESULTS

The viscoelastic hydrogel was successfully injected, and remained translucent with preserved gel properties throughout the postoperative period. The postoperative IOP was unchanged compared to preoperative values. Five of six eyes displayed retinal edema or pigmentary changes centrally while the periphery appeared intact. ERG recordings showed a radical decrease in rod- and cone-derived B-wave amplitudes. Histological examination confirmed varying degrees of edema combined with neuronal cell death within the retinal layers in the central part of the fundus, while the peripheral part appeared intact.

CONCLUSION

Polyalkylimide displays favourable physical properties when used as a vitreous tamponade. However, the hydrogel causes functional and morphological retinal damage when in direct contact with the inner retina. Possible pathological mechanisms include osmotic imbalance and direct toxic effects, and modification of biochemical properties is warranted before clinical use will be possible.

摘要

目的

评估聚烷基酰亚胺作为一种可能的玻璃体填塞剂。

方法

在 6 只色素兔的右眼行 20 号巩膜扁平部玻璃体切除术和后玻璃体脱离。随后向玻璃体腔注入约 1ml 粘性凝胶,聚烷基酰亚胺(Bio-Alcamid)。在术前和术后定期间隔至 28 天,测量全视野 ERG 和眼压(Tonopen)。在第 6 天或第 28 天,处死兔子,对眼睛进行大体检查、拍照,并进行常规显微镜下的组织学检查。

结果

粘性水凝胶成功注射,在整个术后期间保持半透明状态,保留凝胶特性。术后眼压与术前值相比无变化。6 只眼中有 5 只显示中央视网膜水肿或色素改变,而周边部则保持完整。ERG 记录显示杆状和锥状 B 波振幅明显降低。组织学检查证实眼底中央部视网膜各层存在不同程度的水肿,伴有神经元细胞死亡,而周边部保持完整。

结论

聚烷基酰亚胺作为玻璃体填塞剂具有良好的物理性能。然而,当水凝胶与内视网膜直接接触时,会引起功能和形态上的视网膜损伤。可能的病理机制包括渗透失衡和直接毒性作用,在临床应用之前需要对生化性质进行修饰。