Abstract

This study was conducted to examine the bond strength of rebonded orthodontic brackets after adhesive residuals on the surface of the bracket bases were removed by Er,Cr:YSGG lasers. Seventy-six brackets bonded to premolars with a self-etching primer adhesive system were equally divided into four groups after the first debonding with the bracket bases (Group 1) untreated, and treated by (Group 2) Er,Cr:YSGG laser, (Group 3) sandblaster, and (Group 4) Er,Cr:YSGG laser/sandblaster. The treated brackets were rebonded to the new premolars in the same manner as the first-stage experiment. The shear bond strengths were measured, with the bonding/debonding procedures repeated once after the first debonding, and the bracket/adhesive failure modes were evaluated after each debonding. The treated bracket base surfaces were observed under a scanning electron microscopy (SEM). The mean rebond strengths were significantly lower in group 1 than in other groups, and there were no significant differences between the other groups. The mean initial bond strength was significantly higher than the mean rebond strength in group 1 but there was no significant difference between the two in the other three groups. Failures at the bracket-adhesive interface occurred frequently at second debonding in group 1. Under the SEM, residual adhesive was removed from the bracket bases by Er,Cr:YSGG laser, while adhesive remnant was seen underneath the meshwork of the bracket bases and microroughness appeared on the meshwork after sandblasting. Er,Cr:YSGG laser certainly could serve the purpose of promoting the use of recycled orthodontic brackets.

摘要

本研究旨在探讨 Er,Cr:YSGG 激光去除托槽基底表面残留粘结剂后,重新粘结正畸托槽的粘结强度。76 个用自酸蚀粘结剂系统粘结于前磨牙上的托槽,在第一次脱落后,按托槽基底(第 1 组)未处理、用 Er,Cr:YSGG 激光(第 2 组)、喷砂(第 3 组)、Er,Cr:YSGG 激光/喷砂(第 4 组)处理,分为 4 组,然后按与第一阶段相同的方式将处理后的托槽重新粘结于新的前磨牙上。测量剪切粘结强度,在第一次脱落后重复粘结/脱粘结操作一次,每次脱落后评估粘结/脱粘结模式。用扫描电子显微镜(SEM)观察处理后的托槽基底表面。第 1 组的平均再粘结强度显著低于其他组,而其他组之间无显著差异。第 1 组的初始粘结强度显著高于平均再粘结强度,但其他 3 组之间无显著差异。第 1 组在第二次脱落后,托槽/粘结剂界面处的粘结失效较为常见。在 SEM 下,Er,Cr:YSGG 激光从托槽基底去除残留粘结剂,而喷砂后,在托槽基底的网格下可见粘结残留,网格出现微粗糙。Er,Cr:YSGG 激光确实可以促进重复使用正畸托槽。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验