Department of Chemistry, U-3060, University of Connecticut, Storrs, Connecticut 06269-3060, USA.
Langmuir. 2011 Jun 21;27(12):7663-71. doi: 10.1021/la2015034. Epub 2011 May 18.
The synthesis, characterization, and evaluation of a novel polymer-protein conjugate are reported here. The covalent conjugation of high-molecular weight poly(acrylic acid) (PAA) to the lysine amino groups of met-hemoglobin (Hb) resulted in the covalent conjugation of Hb to PAA (Hb-PAA conjugate), as confirmed by dialysis and electrophoresis studies. The retention of native-like structure of Hb in Hb-PAA was established from Soret absorption, circular dichroism studies, and the redox activity of the iron center in Hb-PAA. The peroxidase-like activities of the Hb-PAA conjugate further confirmed the retention of Hb structure and biological activity. Thermal denaturation of the conjugate was investigated by differential scanning calorimetry and steam sterilization studies. The Hb-PAA conjugate indicated an improved denaturation temperature (T(d)) when compared to that of the unmodified Hb. One astonishing observation was that polymer conjugation significantly enhanced the Hb-PAA storage stability at room temperature. After 120 h of storage at room temperature in phosphate-buffered saline (PBS) at pH 7.4, for example, Hb-PAA retained 90% of its initial activity and unmodified Hb retained <60% of its original activity under identical conditions of buffer, pH, and temperature. Our conjugate demonstrates the key role of polymers in enhancing Hb stability via a very simple, efficient, general route. Water-swollen, lightly cross-linked, stable Hb-polymer nanogels of 100-200 nm were produced quickly and economically by this approach for a wide variety of applications.
本文报道了一种新型聚合物-蛋白缀合物的合成、表征和评价。通过透析和电泳研究证实,通过将高分子量聚丙烯酸(PAA)与血红蛋白(Hb)的赖氨酸氨基共价连接,导致 Hb 与 PAA 的共价连接(Hb-PAA 缀合物)。Hb-PAA 保留了 Hb 结构的天然样结构,这从 Soret 吸收、圆二色性研究和 Hb-PAA 中铁中心的氧化还原活性得到证实。Hb-PAA 缀合物的过氧化物酶样活性进一步证实了 Hb 结构和生物活性的保留。通过差示扫描量热法和蒸汽灭菌研究研究了缀合物的热变性。与未修饰的 Hb 相比,Hb-PAA 缀合物的变性温度(T(d))有所提高。一个惊人的观察结果是,聚合物缀合显著提高了 Hb-PAA 在室温下的储存稳定性。例如,在 pH 7.4 的磷酸盐缓冲盐水(PBS)中在室温下储存 120 小时后,Hb-PAA 保留了其初始活性的 90%,而在相同的缓冲液、pH 和温度条件下,未修饰的 Hb 仅保留了其原始活性的<60%。我们的缀合物通过一种非常简单、高效、通用的途径证明了聚合物在增强 Hb 稳定性方面的关键作用。通过这种方法可以快速、经济地制备 100-200nm 的水膨胀、轻度交联、稳定的 Hb-聚合物纳米凝胶,适用于各种应用。