Department of Orthodontics, Noorul Islam College of Dental Sciences, Trivandrum, Kerala India.
Angle Orthod. 2012 Jul;82(4):703-8. doi: 10.2319/072111-460.1. Epub 2011 Oct 19.
To clinically evaluate the alignment efficiency of 0.016-inch coaxial superelastic nickel-titanium (NiTi) and 0.016-inch superelastic NiTi in the lower anterior region over a period of 12 weeks.
A sample of 24 patients requiring lower anterior alignment were included in this single-center, single-operator, double-blind clinical trial and were randomly allocated into two groups of 12 patients. The type of wire selected for each patient was not disclosed to the provider or to the patient. Comparison of pretreatment characteristics of the archwire groups revealed no discrimination between two samples, thus verifying the random allocation of the intervention. An initial alginate impression of the lower arch was followed by impressions at 4-, 8-, and 12-week intervals. Casts were measured using the coordinate measuring machine to denote the degree of alignment. Duplicate readings of the cast series were taken to assess measurement variation.
A statistically significant difference (P < .05) in the mean values of tooth movement demonstrated the superior aligning efficiency of coaxial superelastic NiTi over single-stranded superelastic NiTi in relieving lower anterior crowding. The measurement error recorded was within acceptable limits, with range values within 95% limits of agreement.
Coaxial superelastic NiTi wire proved superior to single-stranded NiTi in its efficiency in relieving lower anterior crowding over a 12-week period.
临床评估 0.016 英寸同轴超弹性镍钛(NiTi)和 0.016 英寸超弹性 NiTi 在 12 周内在下前牙区的排齐效率。
本单中心、单操作、双盲临床试验纳入 24 例需要下前牙排齐的患者,随机分为两组,每组 12 例。每位患者选择的弓丝类型不向医生或患者透露。对弓丝组的预处理特征进行比较,发现两组之间没有差异,从而验证了干预措施的随机分配。首先对下牙弓进行初始藻酸盐印模,然后在 4、8 和 12 周间隔进行印模。使用坐标测量机测量牙模以表示排齐程度。对牙模系列进行重复读数以评估测量变化。
牙齿移动的平均值存在统计学显著差异(P<.05),表明同轴超弹性 NiTi 在缓解下前牙拥挤方面的排齐效率优于单股超弹性 NiTi。记录的测量误差在可接受范围内,范围值在 95%一致性界限内。
在 12 周的时间内,同轴超弹性 NiTi 丝在缓解下前牙拥挤方面的效率优于单股 NiTi。