Harris Orthopaedic Laboratory, Department of Orthopaedic Surgery, Harvard Medical School, Massachusetts General Hospital, 55 Fruit Street, GRJ1126, Boston, MA 02114, USA.
Clin Orthop Relat Res. 2012 Nov;470(11):3077-82. doi: 10.1007/s11999-012-2330-7.
Edge wear is an adverse factor that can negatively impact certain THAs. In some metal-on-metal THAs, it can lead to adverse tissue reactions including aseptic lymphocytic vasculitis-associated lesions and even to pseudotumor formation. In some ceramic-on-ceramic THAs, it can lead to squeaking and/or stripe wear. Edge wear in metal-on-metal and ceramic-on-ceramic THAs can also be associated with accelerated wear across the articulation of these joints.
QUESTIONS/PURPOSES: I asked: Does edge wear occur in metal-on-polyethylene (MOP) articulations? And if so, does it increase joint wear?
I examined the evidence in the literature for edge wear occurring in MOP THA and then assessed the evidence in the literature for data supporting the concept that edge wear in MOP hips could accelerate wear across the articulation over time.
Extensive data in the literature confirm edge wear is common in MOP THA. Surprisingly, the evidence does not support that it accelerates wear across the articulation. In fact, substantial data support the concept that it does not.
These observations suggest, in terms of edge wear accelerating overall wear, MOP articulation may have a privileged position compared to hard-on-hard THA articulations.
边缘磨损是一种不利因素,会对某些全髋关节置换术产生负面影响。在某些金属对金属全髋关节置换术中,它会导致不良的组织反应,包括无菌性淋巴细胞血管炎相关病变,甚至导致假瘤形成。在某些陶瓷对陶瓷全髋关节置换术中,它会导致嘎吱声和/或条纹磨损。金属对金属和陶瓷对陶瓷全髋关节置换术中的边缘磨损也可能与这些关节的关节表面的加速磨损有关。
问题/目的:我提出了以下问题:边缘磨损是否会发生在金属对聚乙烯(MOP)关节中?如果是,它是否会增加关节磨损?
我检查了文献中关于 MOP 全髋关节置换术中发生边缘磨损的证据,然后评估了文献中关于支持 MOP 髋关节边缘磨损可能随时间加速关节表面磨损这一概念的证据。
文献中有大量数据证实边缘磨损在 MOP 全髋关节置换术中很常见。令人惊讶的是,证据并不支持它会加速关节表面的磨损。事实上,大量数据支持这样一种观点,即它不会。
这些观察结果表明,就边缘磨损加速整体磨损而言,MOP 关节可能与硬对硬全髋关节置换术关节相比具有特权地位。